Abstract

Fibers comprising a propylene homopolymer or a copolymer of propylene and at least one of ethylene and one or more unsaturated comonomers exhibit desirable properties. The homopolymers are characterized as having <SUP>13</SUP>C NMR peaks corresponding to a regio-error at about 14.6 and about 15.7 ppm, the peaks of about equal intensity. The copolymers are characterized as (A) comprising at least about 60 weight percent (wt %) of units derived from propylene, and (B) having at least one of the following properties: (i) <SUP>13</SUP>C NMR peaks corresponding to a regio-error at about 14.6 and about 15.7 ppm, the peaks of about equal intensity, (ii) a B-value greater than about 1.4 when the comonomer content of the copolymer is at least about 3 wt %, (iii) a skewness index, S<SUB>ix</SUB>, greater than about -1.20, (iv) a DSC curve with a T<SUB>me </SUB>that remains essentially the same and a T<SUB>max </SUB>that decreases as the amount of comonomer in the copolymer is increased, and (v) an X-ray diffraction pattern that reports more gamma-form crystals than a comparable copolymer prepared with a Ziegler-Natta (Z-N) catalyst.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 27.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A fiber comprising an isotactic propylene homopolymer characterized as having 13 C NMR peaks corresponding to a regio-error at about 14.6 and about 15.7 ppm, the peaks of about equal intensity.

  2. Claim 2Depends on #1

    The fiber of claim 1 further characterized as having substantially isotactic propylene sequences.

  3. Claim 3Depends on #2

    The fiber of claim 2 further comprising a polymer other than an isotactic propylene homopolymer characterized as having 13 C NMR peaks corresponding to a regio-error at about 14.6 and about 15.7 ppm, the peaks of about equal intensity.