US 11,230,641 B2#88205376 Most CitedActiveUnited States (USPTO)Utility

Polyolefin based elastic compositions, methods of manufacturing thereof and articles comprising the same

0Forward Citations (#88205376 Global)
0.0/yrCitation Velocity (#88205376 Global)
0.56Citation PageRank (#88205376 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed herein is a film comprising a polymer blend, the polymer blend comprising a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C. Disclosed herein too is a method of manufacturing a film comprising blending a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole to form a polymer blend; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; and forming the polymer blend into a film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A polymer blend comprising: a first polyolefin elastomer having a weight average molecular weight of 120,000 to 350,000 grams per mole; and a second polyolefin elastomer having a weight average molecular weight of 15,000 to 75,000 grams per mole; wherein the overall melt index of the polymer blend is less than 8 g/10 minutes when measured as per ASTM D1238 at 2.16 kilograms at 190° C.; wherein the first polyolefin elastomer is present in the blend in an amount of greater than 50 wt %, based on the total weight of the blend; wherein the first polyolefin elastomer and the second polyolefin elast

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,041,203 ANonwoven thermoplastic fabric19771,290
US 4,107,364 ARandom laid bonded continuous filament cloth1978316
US 4,116,892 AProcess for stretching incremental portions of an orientable thermoplastic substrate and product thereof1978421
US 4,153,751 AProcess for stretching an impregnated film of material and the microporous product produced thereby1979140
US 4,209,463 APromoting the formation of nitrodiarylamines from nitrohaloarenes, activated aryl amines and sodium carbonates198028
US 4,230,831 APolyethylene blend composition198053
US 4,368,565 AGrooved roller assembly for laterally stretching film1983115
EP 0,100,843 A1Ethylene polymer blend—72
US 4,525,407 AElastic composites1985231
US 4,547,551 AEthylene polymer blends and process for forming film1985178
US 4,720,415 AComposite elastomeric material and process for making the same1988879
US 4,762,890 AMethod of grafting maleic anhydride to polymers1988190
US 4,927,888 AMaleic anhydride graft copolymers having low yellowness index and films containing the same1990176
US 4,950,541 AMaleic anhydride grafts of olefin polymers1990309
US 5,143,679 AMethod for sequentially stretching zero strain stretch laminate web to impart elasticity thereto without rupturing the web1992595
US 5,145,727 AMultilayer nonwoven composite structure1992363
US 5,156,793 AMethod for incrementally stretching zero strain stretch laminate web in a non-uniform manner to impart a varying degree of elasticity thereto1992608
US 5,167,897 AMethod for incrementally stretching a zero strain stretch laminate web to impart elasticity thereto1992923
US 5,169,706 ALow stress relaxation composite elastic material1992443
US 5,178,931 AThree-layer nonwoven laminiferous structure1993267
US 5,188,885 ANonwoven fabric laminates1993293
US 5,504,172 APropylene polymer, propylene copolymer, and propylene elastomer prepared using novel bridged indenyl containing metallocenes1996427
US 5,783,638 AElastic substantially linear ethylene polymers1998249
WO 0,001,745 A1Propylene olefin copolymers—281
US 6,525,157 B2Propylene ethylene polymers2003433
US 2003088228 A1Variable stretch composites and methods of making the composite—58
US 6,610,408 B1TPO blends containing multimodal elastomers200312
WO 2004/020174 A1Device and process for treating flexible web by stretching between intermeshing forming surfaces—18
US 2004222553 A1Method for making a stretch composite—45
WO 2005/090426 A1Catalyst composition comprising shuttling agent for higher olefin multi-block copolymer formation—234

Non-Patent Literature (5)

  • International Search Report for International Application No. PCT/US2016/043317, International Filing Date Jul. 21, 2016, dated Sep. 28, 2016, 6 pages.
  • Markovich et al.; “Development of Gel Permeation Chromatography-Fourier Transform Infrared Spectroscopy for Characterization of Ethylene Based Polyolefin Copolymers”; Polymeric Materials Science and Engineering, vol. 65, 1991, pp. 98-100.
  • U.S. Appl. No. 60/566,2938, filed Mar. 17, 2005.
  • U.S. Appl. No. 60/662,937, filed Mar. 17, 2005.
  • U.S. Appl. No. 60/662,939, filed Mar. 17, 2005.