Elastomer composition for cross-linked olefin elastomer foam
Abstract
A crosslinked olefin elastomer foam has a specific gravity of 0.05 to 0.2, an expansion ratio of 8 to 15, a compression set of 30 to 60% and a tear strength of 1.5 to 2.5 kg/cm. The crosslinked foam is obtained by heating an elastomer composition comprising a specific ethylene/alpha-olefin copolymer, an organic peroxide, a crosslinking auxiliary and a foaming agent. The crosslinked foam has a high expansion ratio, is free from surface roughening attributed to defoaming, realizes a soft touch, exhibits a low compression set and is excellent in mechanical strength (particularly tear strength) and heat resistance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An elastomer composition for crosslinked olefin elastomer foam, comprising: 70 to 95 parts by weight of an ethylene/α-olefin copolymer (A) having a density of 0.88 to 0.92 g/cm 3 and a melt flow rate (measured at 190° C. under a load of 2.16 kg in accordance with ASTM D 1238) of 0.1 to 10 g/10 mm, and 5 to 30 parts by weight of a modified polyolefin (B) obtained by grafting a polyolefin with an unsaturated carboxylic acid or a derivative thereof, provided that the sum of ethylene/α-olefin copolymer (A) and modified polyolefin (B) is 100 parts by weight; an organic peroxide (D); a crosslinking
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗