US 6,720,364 B2#7753068 Most CitedExpiredUnited States (USPTO)Utility

Elastomeric composition for preparing olefinic elastomer crosslinked foam and use thereof

13Forward Citations (#7753068 Global)
0.6/yrCitation Velocity (#13564168 Global)
2.07Citation PageRank (#13741624 Global)
6Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The elastomeric composition for preparing an olefinic elastomer crosslinked foam according to the present invention contains an ethylene/α-olefin copolymer (A) having a specific density and MFR, an organic peroxide (D), a crosslinking assistant (E), a foaming agent (F), an organic metal compound (G), and as necessary, a high pressure low density polyethylene (B) having a specific MFR, and an ethylene/vinyl acetate copolymer (C) having a specific amount of vinyl acetate and a specific MFR. An olefinic elastomer crosslinked foam of the present invention can be obtained by crosslinking and foaming the above composition. Further, another olefinic elastomer crosslinked foam of the present invention can be obtained by a secondary compression of the above crosslinked foam. The footwear part of the present invention is made of these crosslinked foams. The present invention provides an elastomeric composition for preparing an olefinic elastomer crosslinked foam that can provide an olefinic elastomer crosslinked foam having an Asker C hardness of 20 to 80, a low specific gravity, a low compression set, and excellent tear strength and impact resilience; and a crosslinked foam made of this. Fu

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An elastomeric composition for preparing an olefinic elastomer crosslinked foam, comprising: an ethylene/α-olefin copolymer (A) which has a density (ASTM D 1505) of 880 to 920 kg/m 3 , and a melt flow rate (ASTM D 1238, 190° C., 2.16 kg load), MFR 2.16 , of 0.1 to 10 g/10 min; an organic peroxide (D); a crosslinking assistant (E); a foaming agent (F); and an organic metal compound (G) which is a compound of metal selected from Groups 2 to 12 of the periodic table, and having at least two groups containing unsaturated carbon bond and at least one atom selected from oxygen, sulfur and nitrogen p

  2. Claim 2Depends on #1

    The elastomeric composition according to claim 1 further comprising, based on 100 parts by weight of said ethylene/α-olefin copolymer (A), 5 to 100 parts by weight of a high p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Saret(R) Acrylic Coagents, Exton, PA, USA (copies of catalogs for the Sartomer Company).
  • Saret® Acrylic Coagents, Exton, PA, USA (copies of catalogs for the Sartomer Company).