Patents
US 7,189,293 B2#15870490 Most CitedExpiredUnited States (USPTO)Utility

Method of producing annealed wafer and annealed wafer

7Forward Citations (#15870490 Global)
0.4/yrCitation Velocity (#21743713 Global)
1.50Citation PageRank (#22945562 Global)
14Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention is a method of producing an annealed wafer wherein a silicon single crystal wafer having a diameter of 200 mm or more produced by the Czochralski (CZ) method is subjected to a high temperature heat treatment in an atmosphere of an argon gas, a hydrogen gas, or a mixture gas thereof at a temperature of 1100–1350° C. for 10–600 minutes, and before the high temperature heat treatmen, a pre-annealing is performed at a temperature less than the temperature of the high temperature heat treatment, so that the growth of slip dislocations is suppressed by growing oxide precipitates. Thereby, there is provided a method of producing an annealed wafer wherein the generation and growth of slip dislocations generated in a high temperature heat treatment are suppressed and the defect density in the wafer surface layer is lowered even in the case of a silicon single crystal wafer having a large diameter of 200 mm or more, and the annealed wafer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing an annealed wafer wherein a silicon single crystal wafer having a diameter of 200 mm or more produced by the Czochralski (CZ) method is subjected to a high temperature heat treatment in an atmosphere of an argon gas, a hydrogen gas, or a mixture gas thereof at 1100–1350° C. for 10–600 minutes, and before the high temperature heat treatment, a pre-annealing is performed by maintaining the wafer for a period of time at a temperature less than the temperature of the high temperature heat treatment wherein the period of time is sufficient to suppress growth of slip dislocatio

  2. Claim 2Depends on #1

    The method of producing an annealed wafer according to claim 1 , wherein the pre-annealing is performed at least in a single stage for 2 hours or more.

  3. Claim 3Depends on #2

    The method of producing an annealed wafer according to claim 2

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗