Abstract
The present invention provides a silicon single crystal wafer having a diameter of 300 mm or more and having a defect-free layer containing no COP for a depth of 3 μm or more from a surface and a method for producing a silicon single crystal, wherein, when a silicon single crystal having a diameter of 300 mm or more is pulled with nitrogen doping by the CZ method, the crystal is grown with a value of V/G [mm 2 /K·min] of 0.17 or less, where V [mm/min] is a pulling rate, and G [K/mm] is an average of temperature gradient in the crystal along a pulling axis from the melting point of silicon to 1400° C. Thus, there are established conditions for pulling a silicon single crystal and conditions for heat treatment of wafer for obtaining a silicon single crystal wafer having a defect-free layer free from COP for a sufficient depth of the surface layer by pulling a silicon single crystal having a diameter of 300 mm or more, processing the crystal into wafers and subjecting the wafers to the heat treatment.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 15.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A silicon single crystal wafer having a diameter of 300 mm or more and having a defect-free layer containing no COP for a depth of 3 microns or more from a surface.
- Claim 2Independent Claim
A method for producing a silicon single crystal, wherein, when a silicon single crystal having a diameter of 300 mm or more is pulled with nitrogen doping by the Czochralski method, the crystal is grown with a value of V/G [mm2/K min] of 0.17 or less, where V [mm/mm] is a pulling rate, and G [K/mm] is an average of temperature gradient in the crystal along a pulling axis from the melting point of silicon to 1400° C.
- Claim 3Depends on #2
A method for producing a silicon single crystal according to claim 2 , wherein the crystal is grown with a nitrogen concentration of 1×10 13 /cm 3 or more for the nitrogen doping.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- F. Dupret et al., "Global Modelling of Heat Transfer in Crystal Growth Furnaces", Int. J. Heat Mass Transfer, vol. 33, No. 9, pp. 1849-1871, 1990.