Method of improved high K dielectric-polysilicon interface for CMOS devices
Abstract
Methods for forming dielectric layers over polysilicon substrates, useful in the construction of capacitors and other semiconductor circuit components are provided. A self-limiting nitric oxide (NO) anneal of a polysilicon layer such as an HSG polysilicon capacitor electrode, at less than 800° C., is utilized to grow a thin oxide (oxynitride) layer of about 40 angstroms or less over the polysilicon layer. The NO anneal provides a nitrogen layer at the polysilicon-oxide interface that limits further oxidation of the polysilicon layer and growth of the oxide layer. The oxide layer is exposed to a nitrogen-containing gas to nitridize the surface of the oxide layer and reduce the effective dielectric constant of the oxide layer. The process is particularly useful in forming high K dielectric insulating layers such as tantalum pentoxide over polysilicon. The nitridized oxynitride layer inhibits oxidation of the underlying polysilicon layer in a post-treatment oxidizing anneal of the high K dielectric, thus maintaining the oxide layer as a thin layer over the polysilicon layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of fanning a dielectric layer, comprising the steps of: annealing a polysilicon substrate in nitric oxide to form an oxide layer on the polysilicon substrate; nitridizing the oxynitride layer to form a nitride layer on the oxide layer by exposure of the oxide layer to a plasma mixture of nitrogen and helium or nitrogen and argon; and depositing the dielectric layer onto the nitride layer.
- Claim 2Depends on #1
The method of claim 1 , wherein the polysilicon substrate comprises a polysilicon selected from the group consisting of doped polysilicon, undoped polysilicon, and HSG polysilicon.
- Claim 3Depends on #1
The method of claim 1 , wherein the oxide layer is about 40 angstroms or less.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗