Method for improved plasma nitridation of ultra thin gate dielectrics

21Forward Citations (#4015041 Global)
1.0/yrCitation Velocity (#6370681 Global)
2.59Citation PageRank (#9602502 Global)
21Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming a gate dielectric for an integrated circuit device. In an exemplary embodiment of the invention, the method includes forming an initial oxynitride layer upon a substrate material, the oxynitride layer having an initial physical thickness. The initial oxynitride layer is then subjected to a plasma nitridation, the plasma nitridation resulting in final oxynitride layer having a final physical thickness.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 21.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a gate dielectric for an integrated circuit device, the method comprising: forming an initial heavily nitrided oxynitride layer upon a substrate material, said initial heavily nitrided oxynitride layer having an initial thickness; and subjecting said initial heavily nitrided oxynitride layer to a plasma nitridation, said plasma nitridation resulting in a final oxynitride layer, said final oxynitride layer having a final thickness, wherein said final oxynitride layer has an equivalent oxide thickness of less than 15 angstroms and a nitrogen dosage of at least 2.0×10 15 ato

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said final thickness exceeds said initial thickness by less than 5 angstroms.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein said final thickness is less than 20 angstroms.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
US 2006138594 A1Method of improved high K dielectric - polysilicon interface for CMOS devices—0
US 7,129,128 B2Method of improved high K dielectric-polysilicon interface for CMOS devices20063
US 2007007604 A1Method for forming a dielectric layer and related devices—0
US 7,470,583 B2Method of improved high K dielectric-polysilicon interface for CMOS devices20083
US 2007275322 A1Negative-working radiation-sensitive compositions and imageable materials—16
US 2004224462 A1Method for forming a dielectric layer and related devices—0
US 2007173069 A1Method of forming insulating layer of semiconductor device—4
US 2004005748 A1Methods of forming a gate insulating layer in an integrated circuit device in which the gate insulating layer is nitrified and then annealed to cure defects caused by the nitridation process—11
US 2006141698 A1Method of improved high K dielectric - polysilicon interface for CMOS devices—3
US 8,835,275 B2Semiconductor devices having nitrided gate insulating layer and methods of fabricating the same20145
US 2008032512 A1Method forming silicon oxynitride gate dielectric layer with uniform nitrogen concentration—10
US 7,511,321 B2Method for forming a dielectric layer and related devices20090
US 7,101,811 B2Method for forming a dielectric layer and related devices20063
US 7,227,209 B2Method of improved high K dielectric—polysilicon interface for CMOS devices20070
US 2003052358 A1Method of improved high K dielectric - polysilicon interface for CMOS devices—39

Non-Patent Literature (2)

  • Gusev, E.P.; Lu, H.C.; Garfunkel, E. L.; Gustafsson, T.; and Green, M. L., "Growth and Characterization of Ultrathin Nitrided Silicon Oxide Film," IBM Journal of Research and Development, vol. 43, No. 3, 1999, pp. 1-22.
  • Lucovsky, G., "Ultrathin Nitrided Gate Dielectrics: Plasma Processing, Chemical Characterization, Performance and Reliability," IBM Journal of Research & Development, vol. 43, No. 3, 1999, pp. 1-27.