Cationically curable dental materials
Abstract
The invention relates to a polymerizable dental material containing: (a) 3 to 80 wt. % of one or more cationically curable monomers; (b) 3 to 90 wt. % of one or more radio-opaque fillers; (c) 0.01 to 25 wt. % of initiators, retarders and/or accelerators, and; (d) 0 to 25 wt. % of auxiliary agents, whereby the cited percentages each refer to the total weight of the material. Filler (b) is produced by means of a melting method and is selected so that it has a refractive index of n D =1.49–1.54, so that the viscosity of the polymerizable dental material, after a period of at least 9 months during which it was stored at a temperature ranging from 20 to 25° C., has a value of +/−50 % of the initial value measured 24 hours after the polymerizable dental material was produced, and so that the polymerizable dental material has a reactivity of the type that, once polymerization is initiated, the amount of the maximum heat flux generated by the dental material equals at least 0.8 mW/mg, and this maximum heat flux is attained within a period of no longer than 60s.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 6.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for the preparation of a polymerizable dental material, the process comprising: (a) preparing a filler from individual components by a melting process at a temperature of at least 1550° C.; (b) grinding the filler obtained in (a) to a particle size of 0.1–15μm; (c) surface-treating the filler obtained in (b); and (d) incorporating the surface-treated filler in a matrix comprising: (i) cationically curable monomers; and (ii) initiators, retarders, accelerators, auxiliary agents, or combinations thereof; wherein the filler is an X-ray opaque filler comprising at least 65 weight % of Si
- Claim 2Depends on #1
The process of claim 1 , wherein the melting process is carried out at a temperature of at least 1600° C.
- Claim 3Independent Claim
The proce
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (29)
Non-Patent Literature (5)
- Billmeyer, Jr., Textbook of Polymer Science, Third Edition, John Wiley & Sons, New York, (1984), Title page, Publication page, and pp. 82-83 (4 pgs total).
- Bowen et al., "121:18236p An esthetic glass-ceramic for use in composite restoration inserts" Chemical Abstracts, 1-Pharmacology, Weisberger, Ed., vol. 121, No. 15, 2 Publication pages. and pp. 1 and 562 (4 pp. total) (Oct. 10, 1994).
- de Gee et al., "Occlusal wear stimulation with the ACTA wear machine," Journal of Dentistry; Butterworth-Heinemann Ltd., Oxford, UK, vol. 22, Suppl. No. 1, Title page, Publication page, Table of Contents, and pp. S21-S27 (9 pp. total) (1994).
- Harrysson et al., "Glass Formation in the System Y<SUB>2</SUB>O<SUB>3</SUB>-Al<SUB>2</SUB>O<SUB>3</SUB>-SiO<SUB>2 </SUB>Under Conditions of Laser Melting," Journal of European Ceramic Society, Elsevier Science Limited, England, vol. 14, Title page, Publication page, Table of Contents, and pp. 377-38
- Harrysson et al., “Glass Formation in the System Y2O3-Al2O3-SiO2 Under Conditions of Laser Melting,” Journal of European Ceramic Society, Elsevier Science Limited, England, vol. 14, Title page, Publication page, Table of Contents, and pp. 377-381 (8 pp. total) (1994).