US 6,953,601 B2#3432241 Most CitedExpiredUnited States (USPTO)Utility

Synthetic free layer for CPP GMR

23Forward Citations (#3432241 Global)
1.1/yrCitation Velocity (#5779676 Global)
3.87Citation PageRank (#5025854 Global)
12Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Reduction of the free layer thickness in GMR devices is desirable in order to meet higher signal requirements, besides improving the GMR ratio itself. However, thinning of the free layer reduces the GMR ratio and leads to poor thermal stability. This problem has been overcome by making AP 2 from an inverse GMR material and by changing the free layer from a single uniform layer to a ferromagnetic layer AFM (antiferromagnetically) coupled to a layer of inverse GMR material. Examples of alloys that may be used for the inverse GMR materials include FeCr, NiFeCr, NiCr, CoCr, CoFeCr, and CoFeV. Additionally, the ruthenium layer normally used to effect antiferromagnetic coupling can be replaced by a layer of chromium. A process to manufacture the structure is also described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 23.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process to manufacture a synthetically pinned CPP SV magnetic read head, comprising: providing a substrate and depositing thereon a seed and then depositing a layer of antiferromagnetic material on said seed layer; on said layer of antiferromagnetic material, depositing a first layer of an inverse GMR material; depositing a first layer of chromium on said first layer; on said first layer of chromium, depositing a second layer, of cobalt-iron; then depositing a copper spacer layer on said second layer; on said copper spacer layer, depositing a third layer, of low coercivity ferromagnetic mate

  2. Claim 2Independent Claim

    The process described in

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 23 total)

PatentTitleYearCitations
US 7,881,018 B2Differential current perpendicular to plane giant magnetoresistive sensor structure having improved robustness against spin torque noise201115
US 7,295,409 B2CPP giant magnetoresistive element with particular bulk scattering coefficient20072
US 7,446,982 B2Pinning structure with trilayer pinned layer20087
US 7,099,122 B2Spin polarization enhancement artificial magnet200615
US 2005128651 A1Spin polarization enhancement artificial magnet—10
US 7,199,983 B2Magnetoresistive device utilizing a magnetoresistance effect for reading magnetic information20070
US 9,218,826 B1Tuned horizontally symmetric magnetic stack20153
US 2006044706 A1Sensor with in-stack bias structure providing exchange stabilization—9
US 7,495,303 B2Magnetic elements with spin engineered insertion layers and MRAM devices using the magnetic elements20090
US 2006007608 A1Synthetic free layer for CPP GMR—0
US 2004228045 A1CPP giant magnetoresistive element—40
DE 102010055754 A1Magnetoresistive sensor for measuring external magnetic field, has measuring layer and reference layer that are separated by nonmagnetic separation layer, and reference layer to adjust anisotropy of region along magnetization direction—2
US 7,324,312 B2Sensor with in-stack bias structure providing exchange stabilization20082
US 2009059437 A1Differential current perpendicular to plane giant magnetoresistive sensor structure having improved robustness against spin torque noise—10
US 7,369,427 B2Magnetic elements with spin engineered insertion layers and MRAM devices using the magnetic elements2008101