Method of forming haze-free BST films
Abstract
Described herein is a method for producing a haze-free (Ba, Sr)TiO 3 (BST) film, and devices incorporating the same. In one embodiment, the BST film is made haze-free by depositing the film with a substantially uniform desired crystal orientation, for example, (100), preferably by forming the film by metal-organic chemical vapor deposition at a temperature greater than about 580° C. at a rate of less than about 80 Å/min, to result in a film having about 50 to 53.5 atomic percent titanium. In another embodiment, whereby the BST film serves as a capacitor for a DRAM memory cell, a desired {100} orientation is induced by depositing the bottom electrode over a nucleation layer of NiO, which gives the bottom electrode a preferential {100} orientation. BST is then grown over the {100} oriented bottom electrode also with a {100} orientation. A nucleation layer of materials such as Ti, Nb and Mn can also be provided over the bottom electrode and beneath the BST film to induce smooth, haze-free BST growth. Haze-free BST film can also be favored by forming the bottom electrode at high temperatures close to those used for BST deposition, and without a vacuum break between the bottom electrode
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for forming a substantially haze-free BST film, comprising: supplying BST sources into a chamber; heating the chamber to a temperature above 600° C.; and depositing the BST film at a rate of between about 10 and about 100 Å/mm while maintaining the chamber at a temperature above 600° C., wherein the resulting BST film comprises about 52 to 53 atomic percent titanium.
- Claim 2Depends on #1
The method of claim 1 , wherein the BST film is deposited at a rate of less than about 80 Å/min.
- Claim 3Depends on #1
The method of claim 1 , wherein the chamber is heated to a temperature of up to about 680° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (28)
Non-Patent Literature (5)
- C. Basceri, "An Important Failure Mechanism in MOCVD (Ba Sr) TiO Thin Films: Resistance Degradation," Ferroelectric Thin Films IV, Materials Research Society, 1998, pp. 9-14.
- C. Basceri, "An Important Failure Mechanism in MOCVD (Ba,Sr) TiO Thin Films: Resistance Degradation", Ferroelectric Thin Films IV, Materials Research Society, 1998, pp. 9-14.
- C. Basceri, "An Important Failure Mechanism in MOCVD (Ba,Sr) TiO<SUB>3 </SUB>Thin Films: Resistance Degradation",Ferroelectric Thin Films IV, Materials Research Society, Symposium Proceedings vol. 493, 1998, pp. 9-14.
- Chung Ming Chu and Pan Lin, "Electrical Properties and Crystal Structure of a (Ba Sr) TiO3 Films Prepared at Low Temperatures on a LaNiO3 Electrode by Radio-Frequency Magnetron Sputtering," Appl. Phys. Lett., vol. 70 (2), Jan. 13, 1997, pp. 249-251.
- Chung Ming Chu and Pang Lin, "Electric Properties and Crystal Structure of a (Ba,Sr)TiO<SUB>3 </SUB>Films Prepared at Low Temperatures on a LaNiO<SUB>3 </SUB>Electrode by Radio-Frequency Magnetron Sputtering", Appl. Phys. Lett., vol. 70 (2), 13 Jan. 1997, pp. 249-51.