Abstract

Described herein is a method for producing a haze-free (Ba, Sr)TiO 3 (BST) film, and devices incorporating the same. In one embodiment, the BST film is made haze-free by depositing the film with a substantially uniform desired crystal orientation, for example, (100), preferably by forming the film by metal-organic chemical vapor deposition at a temperature greater than about 580° C. at a rate of less than about 80 Å/min, to result in a film having about 50 to 53.5 atomic percent titanium. In another embodiment, where the BST film serves as a capacitor for a DRAM memory cell, a desired {100} orientation is induced by depositing the bottom electrode over a nucleation layer of NiO, which gives the bottom electrode a preferential {100} orientation. BST is then grown over the {100} oriented bottom electrode also with a {100} orientation. A nucleation layer of materials such as Ti, Nb and Mn can also be provided over the bottom electrode and beneath the BST film to induce smooth, haze-free BST growth. Haze-free BST film can also be favored by forming the bottom electrode at high temperatures close to those used for BST deposition, and without a vacuum break between the bottom electrode a

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A thin film structure, comprising: a substrate; an electrode formed over said substrate; a nucleation layer for improving the uniformity of a crystal orientation of a BST film formed thereon, wherein said nucleation layer consists essentially of a donor or acceptor dopant material, said nucleation layer being formed over said electrode; and a BST film over the nucleation layer having a substantially uniform crystal orientation.

  2. Claim 2Depends on #1

    The thin film structure of claim 1 , wherein the the donor or acceptor dopant material is selected from the group consisting of Ti, Nb and Mn.

  3. Claim 3Depends on #1

    The thin film structure of claim 1 , wherein the donor or acceptor dopant material is a metal.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 5,185,689 ACapacitor having a ruthenate electrode and method of formation1993120
US 5,335,138 AHigh dielectric constant capacitor and method of manufacture1994346
JP H06333772 AThin film capacitor and manufacture thereof—18
US 5,406,445 AThin film capacitor and method of manufacturing the same199527
WO 9,525,340 A1Thin film capacitors on gallium arsenide substrate and process for making the same—7
US 5,506,166 AMethod for forming capacitor compatible with high dielectric constant materials having a low contact resistance layer1996248
US 5,581,436 AHigh-dielectric-constant material electrodes comprising thin platinum layers1996129
US 5,717,234 AMetalorganic chemical vapor deposition of (ba1-x Srx)RuO3 /Ba1-x Srx)TiO3 /(Ba1-x SRx)RuO3 capacitors for high dielectric materials199824
US 5,781,404 AElectrode interface for high-dielectric-constant materials199837
US 5,783,253 AMethod for forming a dielectric film and method for fabricating a capacitor using the same199872
US 5,822,175 AEncapsulated capacitor structure having a dielectric interlayer199864
US 5,889,299 AThin film capacitor199960
US 6,010,931 APlanarization technique for DRAM cell capacitor electrode200067
US 6,117,482 AMethod and apparatus for monitoring CVD liquid source for forming thin film with high dielectric constant20008
US 6,136,639 ASemiconductor memory device and method for fabricating the same200018
US 6,238,966 B1Semiconductor memory device and method for fabricating the same200112
US 6,277,436 B1Liquid delivery MOCVD process for deposition of high frequency dielectric materials200191
US 6,285,051 B1Semiconductor memory device and method for fabricating the same200122
US 6,319,764 B1Method of forming haze-free BST films200113
US 6,339,527 B1Thin film capacitor on ceramic200234

Non-Patent Literature (3)

  • C. Basceri, "An Important Failure Mechanism in MOCVD (Ba,Sr) TiO Thin Films: Resistance Degradation", Ferroelectric Thin Films IV, Materials Research Society, 1998, pp. 9-14.
  • Hiromi Itoh et al., "Integration of BST Thin Film for Dram Fabrication", Integrated Ferroelectrics, 1995, vol. 11, pp. 101-109.
  • Joo, "Fabrication and Characterization of MOCVD (Ba, Sr)TiO3 Thin Films for High Density Capacitors", Proceeding of 1997 5th International Conference an VLSI and CAD, The Secretariat of ICVC '97, 1997.