A preferred, non-destructive method for characterizing sputter target cleanliness includes the steps of sequentially irradiating the test sample with sonic energy predominantly of target sputter track areas; detecting echoes induced by the sonic energy; and discriminating texture-related backscattering noise from the echoes to obtain modified amplitude signals. These modified amplitude signals are compared with one or more calibration values so as to detect flaw data points at certain positions or locations where the comparison indicates the presence of at least one flaw. Most preferably, groups of the flaw data pixels corresponding to single large flaws are bound together so as to generate an adjusted set of flaw data points in which each group is replaced with a single, most significant data point. The adjusted set of flaw data point is used to calculate one or more cleanliness factors, or to plot a histogram, which characterizes the cleanliness of the sample.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 33 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A non-destructive method for characterizing a test sample of a sputter target material defining a surface, said method using one or more calibration values and comprising the steps of: a) sequentially irradiating the test sample with sonic energy at a plurality of positions on the surface; b) detecting echoes induced by the sonic energy; c) discriminating texture-related backscattering noise from the echoes to obtain modified amplitude signals; d) comparing the modified amplitude signals with the one or more calibration values to detect i) flaw data points at certain positions of the plurality

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (33)

PatentTitleYearCitations
US 2,790,216 AMethod and apparatus for the continuous casting of metal195764
US 4,054,173 AApparatus for producing completely recrystallized metal sheet197740
US 4,568,007 ARefractory shroud for continuous casting198636
EP 0,211,401 B1N+ amorphous silicon thin film transistors for matrix addressed liquid crystal displays19924
US 5,160,388 AProcess for producing cathodes for cathodic sputtering based on aluminium-silicon alloys199230
US 5,369,063 AMolten metal filter medium and method for making same199425
EP 0,418,846 B1Method for fabricating a liquid crystal display and display made by said method19954
US 5,406,850 AMethod of non-destructively testing a sputtering target199536
EP 0,467,659 B1A reflective-type liquid crystal display device and method for producing same19964
EP 0,412,843 B1Liquid crystal display device of optical writing type19964
US 5,559,614 ALiquid crystal display with integral heater and method of fabricating same1996232
EP 0,561,161 B1Method of producing glass panels for liquid crystal display19974
US 5,636,681 AProcess and apparatus for casting metal strip199731
WO 9,730,348 A1Ultrasonic sputtering target testing method—6
US 5,738,767 ASubstrate handling and processing system for flat panel displays199855
EP 0,665,193 B1Substrate handling and processing system for flat panel displays19983
US 5,827,409 AMethod and apparatus for forming thin film for liquid crystal display199855
US 5,887,481 ACathode sputtering targets with a low level of particle emission, precursors of these targets, and processes for obtaining them199930
US 5,943,559 AMethod for manufacturing liquid crystal display apparatus with drain/source silicide electrodes made by sputtering process199930
US 5,955,673 ACathode sputtering targets selected by ultrasonic inspection for their low level of particle emission199923
US 5,989,782 AMethod for producing liquid crystal display device199914
US 6,001,227 ATarget for use in magnetron sputtering of aluminum for forming metallization films having low defect densities and methods for manufacturing and using such target199939
WO 9,964,854 A1Method and apparatus for quantitative sputter target cleanliness characterization—14
US 6,017,779 AFabrication method for a thin film semiconductor device, the thin film semiconductor device itself, liquid crystal display, and electronic device2000100
US 6,020,946 ADry processing for liquid-crystal displays using low energy ion bombardment200082
US 6,019,657 ADual-layer metal for flat panel display200029
WO 0,015,863 A1Low temperature sputter target bonding method and target assemblies produced thereby—30
US 6,057,557 ASemiconductor substrate semiconductor device and liquid crystal display device200043
US 6,139,701 ACopper target for sputter deposition200062

Non-Patent Literature (5)

  • Abburi, M. et al., "Low-Defect Target Metallurgy Development for sub-0.18 mum Al-based Interconnects," Solid State Technology, Dec. 1999, vol. 42, pp. 55-58, Solid State Technology.
  • Akari, K. et al., "Reduction in Macroparticles During the Deposition of TiN Films Prepared by Arc Ion Plating," Surface and Coatings Technology, 1990, 43/44, pp. 312-323, Elsevier Sequoia, The Netherlands.
  • Anderson, H.M. et al., "Particulate Generation in Silane / Ammonia RF Discharges," J. Applied Physics, May 1, 1990, vol. 67, No. 9, pp. 3999-4011, American Institute of Physics.
  • Anderson, L., "A New Technique for Arc Control in DC Sputtering," Society of Vacuum Coaters 35<SUP>th </SUP>Annual Technical Conference Proceedings, 1992, pp. 325-329.
  • Bailey, R.S. et al., "Particle Emission from Al<SUB>2</SUB>O<SUB>3 </SUB>Doped Aluminum Targets During Sputtering Deposition," VMIC Conference, ISMIC, Jun. 7-8, 1994, p. 317.