US 6,838,375 B2#10801173 Most CitedExpiredUnited States (USPTO)Utility

Buried digit line stack and process for making same

10Forward Citations (#10801173 Global)
0.5/yrCitation Velocity (#17443396 Global)
1.63Citation PageRank (#20087358 Global)
19Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process of making a buried digit line stack is disclosed. The process includes forming a silicon-lean metal silicide first film over a polysilicon plug, followed by a silicide compound barrier second film. The silicide compound barrier second film is covered with a refractory metal third film. A salicidation process causes the first film to salicide with the polysilicon plug. In one embodiment, all the aforementioned deposition processes are carried out by physical vapor deposition (“PVD”).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process comprising: physical vapor deposition (PVD) forming a refractory metal silicide first film above a conductive plug; forming a refractory metal silicide nitride second film above the refractory metal silicide first film; and PVD forming a refractory metal third film above the refractory metal silicide nitride second film.

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein forming the first film, forming the second film, and forming the third film are carried out in a single tool.

  3. Claim 3Depends on #1

    The process according to claim 1 , wherein the conductive plug includes a characteristic dimension, and wherein PVD forming a refractory metal third film is carried out under conditions to cause an average grain size therein, wherein the average grain size is larger than the conductive plug characteristic dimension.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 5,392,189 ACapacitor compatible with high dielectric constant materials having two independent insulative layers and the method for forming same1995333
US 5,717,250 ASputter and CVD deposited titanium nitride barrier layer between a platinum layer and a polysilicon plug199898
US 5,770,515 AMethod of in-situ wafer cooling for a sequential WSI/alpha -Si sputtering process199815
US 5,846,881 ALow cost DRAM metallization199846
US 5,892,254 AIntegrated circuit capacitors including barrier layers having grain boundary filling material199959
US 6,017,818 AProcess for fabricating conformal Ti-Si-N and Ti-B-N based barrier films with low defect density2000151
US 6,057,231 AMethod for improved metal fill by treatment of mobility layers200040
US 6,162,671 AMethod of forming capacitors having high dielectric constant material200025
US 6,174,806 B1High pressure anneals of integrated circuit structures200121
US 2001001717 A1Method of manufacturing a semiconductor integrated circuit device—18
US 6,258,719 B1Intermetallic aluminides and silicides articles, such as sputtering targets, and methods of making same20017
US 2001042920 A1Semiconductor device—14
US 6,455,424 B1Selective cap layers over recessed polysilicon plugs200277
US 6,482,735 B1Method for improved metal fill by treatment of mobility layers200223
US 6,495,471 B2Etching process using a buffer layer20025
US 6,524,952 B1Method of forming a titanium silicide layer on a substrate200356
US 6,531,730 B2Capacitor compatible with high dielectric constant materials having a low contact resistance layer and the method for forming same200324
US 6,614,116 B1Buried digit line stack and process for making same20035
US 6,680,246 B2Process for forming a nitride film200411