Abstract
A CVD process for Ti--Si--N or Ti--B--N films wherein a single feed gas (preferably TDMAT) serves as the source for titanium and nitrogen, and another feed gas is used as the source for silicon or boron. This avoids gas-phase particulate nucleation while providing good conformality. When the required thickness has been deposited, the silicon or boron feed gas continues to flow for some time after the titanium/nitrogen or titanium/boron source gas has been turned off. This results in a Ti--N film with a Si-rich or B-rich surface, which is conformal and has a low defect density. In a second embodiment, a single feed gas, such as TDMAT, is thermally decomposed to form a Ti--N layer. A post-deposition anneal is performed in a gas which supplies silicon or boron, incorporating these materials into the layer. The incorporation of silicon or boron into the layer minimizes the absorption of oxygen into the films, and therefore stabilizes the resulting films. The Si-rich or boron-rich surfaces are also helpful in wetting Al and enhancing adhesion to Cu, therefore are advantageous for advanced metallization application. Compared with the sputtering method, this invention offers a process for
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 151.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of forming a thin film, comprising the steps of: (a.) providing a substrate which includes at least one substantially monolithic body of semiconductor material; (b.) depositing a conformal layer by CVD in an atmosphere which includes titanium and nitrogen; (c.) after depositing said conformal layer, exposing said conformal layer to an atmosphere which contains silicon or boron at a temperature greater than or equal to 350 C. but less than 500 C.; wherein said step (c.) produces a silicon- or boron-rich surface on said conformal layer.
- Claim 2Depends on #1
The method of claim 1, wherein said step (c.) follows immediately after step (b.), with no intervening steps.
- Claim 3Depends on #1
The method of claim 1, wherein said step (b.) utilizes an atmosphere which includes silicon or boron.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 151 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (4)
- J. Ryan et al, "The Preparation and Characterization of Titanium Boride Films", Thin Solid Films, vol. 153, pp. 329-339, Dec. 1987.
- J. Ryan et al, The Preparation and Characterization of Titanium Boride Films , Thin Solid Films, vol. 153, pp. 329 339, Dec. 1987.
- S. Reid et al, "Ti-Si-N Diffusion Barriers Between Silicon and Copper", IEEE Electron Device Letters, vol. 15, No. 8, pp. 298-300, Aug. 1994.
- S. Reid et al, Ti Si N Diffusion Barriers Between Silicon and Copper , IEEE Electron Device Letters, vol. 15, No. 8, pp. 298 300, Aug. 1994.