US 6,815,344 B2#97845348 Most CitedExpiredUnited States (USPTO)Utility

Methods of forming an electrically conductive line

0Forward Citations (#97845348 Global)
0.0/yrCitation Velocity (#97845348 Global)
0.56Citation PageRank (#97845348 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of forming a crystalline phase material includes, a) providing a stress inducing material within or operatively adjacent a crystalline material of a first crystalline phase; and b) annealing the crystalline material of the first crystalline phase under conditions effective to transform it to a second crystalline phase. The stress inducing material preferably induces compressive stress within the first crystalline phase during the anneal to the second crystalline phase to lower the required activation energy to produce a more dense second crystalline phase. Example compressive stress inducing layers include SiO 2 and Si 3 N 4 , while example stress inducing materials for providing into layers are Ge, W and Co. Where the compressive stress inducing material is provided on the same side of a wafer over which the crystalline phase material is provided, it is provided to have a thermal coefficient of expansion which is less than the first phase crystalline material. Where the compressive stress inducing material is provided on the opposite side of a wafer over which the crystalline phase material is provided, it is provided to have a thermal coefficient of expansion which is gr

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming an electrically conductive line comprising: forming a semiconductive material over a substrate; forming a refractory metal silicide over and in ohmic electrical connection with the semiconductive material, the refractory metal silicide having a first crystalline phase and having a first thermal coefficient of expansion as initially formed; providing a compressive stress inducing material operably adjacent the refractory metal silicide to lower an energy of activation for transformation of the first crystalline phase to a second crystalline phase, the compressive stress indu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 4,337,476 ASilicon rich refractory silicides as gate metal198248
US 4,378,628 ACobalt silicide metallization for semiconductor integrated circuits1983105
US 4,568,565 ALight induced chemical vapor deposition of conductive titanium silicide films198692
US 4,897,368 AMethod of fabricating a polycidegate employing nitrogen/oxygen implantation1990106
US 4,971,655 AProtection of a refractory metal silicide during high-temperature processing using a dual-layer cap of silicon dioxide and silicon nitride1990118
US 5,240,739 AChemical vapor deposition technique for depositing titanium silicide on semiconductor wafers1993102
JP H06139056 AProgram rewriting device for data processor—1
US 5,376,405 AChemical vapor deposition technique for depositing titanium silicide on semiconductor wafers1994102
US 5,470,794 AMethod for forming a silicide using ion beam mixing199573
US 5,593,924 AUse of a capping layer to attain low titanium-silicide sheet resistance and uniform silicide thickness for sub-micron silicon and polysilicon lines199760
US 5,608,266 AThin film for a multilayer semiconductor device for improving thermal stability and a method thereof199746
US 5,665,646 AMethod for manufacturing semiconductor device with low electric resistance silicide layer on silicon surface199762
US 5,739,573 ASemiconductor device with improved salicide structure and a method of manufacturing the same1998117
US 5,828,131 ALow temperature formation of low resistivity titanium silicide199850
US 5,874,351 ASputtered metal silicide film stress control by grain boundary stuffing199936
US 6,054,387 AMethod for forming a silicide region200021
US 6,090,708 AMethod of forming a crystalline phase material, electrically conductive line and refractory metal silicide200023
US 6,376,372 B1Approaches for mitigating the narrow poly-line effect in silicide formation200228

Non-Patent Literature (5)

  • Hiung, et al. The Influence of Ge-Implantation on the Electrical Characterisdes of the Ultra-Shallow . . . IEEE Electron Device Letters, vol. 17, No. 3, Mar. 1996, pp. 88-90.
  • Ilderem, V., et al., "Optimized Deposition Parameters For Low Pressure Chemical Vapor Deposled Silioide", Massachusetts Institute of Technology, vol. 135, No. 10, pp. 2590-2596 (Feb. 1988).
  • Ma et al., "Manipulation of the Ti/Si reaction path by introducing an amorphous Ge interlayer", 4<th >international conference on Solid-state and Integrated circuit technology Proceedings, 1995, pp. 35-37.
  • Ma et al., "Manipulation of the Ti/Si reaction path by introducing an amorphous Ge interlayer", 4th international conference on Solid-state and Integrated circuit technology Proceedings, 1995, pp. 35-37.
  • Nagabushinam, R.V., et al., "Kinetics And Mechanism Of The C49 to C54 Titanium Disilicide Phase Transformation Formation In Nitogen Ambient", 5 pages (Nov. 1995).