Patents
US 6,090,708 A#3502154 Most CitedExpiredUnited States (USPTO)Utility

Method of forming a crystalline phase material, electrically conductive line and refractory metal silicide

23Forward Citations (#3502154 Global)
0.9/yrCitation Velocity (#8176386 Global)
2.77Citation PageRank (#8624069 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a crystalline phase material includes providing a stress inducing material on a substrate and, after providing the stress inducing material on the substrate, depositing a crystalline phase material over the substrate in a substantially continuous manner and changing deposition temperature at least once during the depositing, and forming the second crystalline phase of the crystalline phase material. In accordance another aspect, a method is performed by providing a stress inducing material on a substrate and, after providing the stress inducing material on the substrate, forming a crystalline phase material over the substrate in at least two discrete crystalline phase material depositions, a later of the depositions being conducted at a different temperature from an earlier of the depositions and forming the second crystalline phase of the crystalline phase material. In another aspect, a method is performed by forming a refractory metal silicide layer of C54 crystalline phase on a substrate, and depositing refractory metal silicide material onto the C54 refractory metal silicide layer with the C54 crystalline phase being induced into the refractory metal silicid

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 23.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a second crystalline phase of a crystalline phase material capable of first and second crystalline phases, where said first and second phases have different densities, the method comprising: providing a stress inducing material on a substrate; and after providing the stress inducing material on the substrate, depositing a crystalline phase material over the substrate in a substantially continuous manner and changing deposition temperature at least once during the depositing, and forming the second crystalline phase of the crystalline phase material.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the second density is greater than the first density.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the second density is greater than the first density, and the stress inducing material imparts compressive stress during th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Ilderem, V., et al., "Optimized Deposition Parameters For Low Pressure Chemical Vapor Deposited Titanium Silicide", Massachusetts Institute of Technology, vol. 135, No. 10, pp. 2590-2596 (Feb. 1988).
  • Ilderem, V., et al., Optimized Deposition Parameters For Low Pressure Chemical Vapor Deposited Titanium Silicide , Massachusetts Institute of Technology , vol. 135, No. 10, pp. 2590 2596 (Feb. 1988).
  • Nagabushnam, R.V., "Kinetics And Mechanism Of The C49 to C54 Titanium Disilicide Phase Transformation Formation In Nitrogen Ambient", 5 Pages (Nov. 1995).
  • Nagabushnam, R.V., Kinetics And Mechanism Of The C49 to C54 Titanium Disilicide Phase Transformation Formation In Nitrogen Ambient , 5 Pages (Nov. 1995).