A new method for combining magnesium oxide, MgO, and magnesium dihydrogen phosphate to form an inexpensive compactible ceramic to stabilize very low solubility metal oxides, ashes, swarfs, and other iron or metal-based additives, to create products and waste forms which can be poured or dye cast, and to reinforce and strengthen the ceramics formed by the addition of fibers to the initial ceramic mixture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 26.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A room temperature process for producing a compactible ceramic from powders, the process comprising: a) combining MgO, and magnesium dihydrogen phosphate dihydrate to create a homogeneous mixture; and b) contacting the mixture with water to form a slurry wherein the slurry sets within an hour.

  2. Claim 2Depends on #1

    The process as recited in claim 1 wherein the mixture is mixed with waste powder prior to contacting the mixture with water.

  3. Claim 3Depends on #2

    The process as recited in claim 2 wherein the waste powder is a high volume waste selected from the group consisting of hazardous wastes, low solubility metal oxides having a pK sp of ˜15 to 25, ceramic powders, ashes, red mud, sand, swarfs, lateritic soils, mineral wastes, and the same with traces of oils or greases, or combinations thereof.