A method of stabilizing a waste in a chemically bonded phosphate ceramic (CBPC). The method consists of preparing a slurry including the waste, water, an oxide binder, and a phosphate binder. The slurry is then allowed to cure to a solid, hydrated CBPC matrix. Next, bound water within the solid, hydrated CBPC matrix is removed. Typically, the bound water is removed by applying heat to the cured CBPC matrix. Preferably, the quantity of heat applied to the cured CBPC matrix is sufficient to drive off water bound within the hydrated CBPC matrix, but not to volatalize other non-water components of the matrix, such as metals and radioactive components. Typically, a temperature range of between 100° C.-200° C. will be sufficient. In another embodiment of the invention wherein the waste and water have been mixed prior to the preparation of the slurry, a select amount of water may be evaporated from the waste and water mixture prior to preparation of the slurry. Another aspect of the invention is a direct anyhydrous CBPC fabrication method wherein water is removed from the slurry by heating and mixing the slurry while allowing the slurry to cure. Additional aspects of the invention are cer

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of stabilizing a radioactive waste in chemically bonded phosphate ceramic comprising: preparing a slurry comprising the radioactive waste, water, an oxide binder and a phosphate binder, wherein the oxide binder is MgO; allowing the slurry to cure to a solid hydrated chemically bonded phosphate ceramic matrix; and removing bound water from the solid hydrated chemically bonded phosphate ceramic matrix, wherein the hydrated ceramic matrix is heated to a select temperature between a lower first temperature where the bound water begins to be driven from the hydrated ceramic matrix and a hi

  2. Claim 2Depends on #1

    The method of claim 1 wherein the waste and the water have been mixed prior to the preparation of the slurry and further comprising removing a select amount of water

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
US 3,416,888 AMethod for preparing spheroidal alumina196816
US 4,351,749 AMolecular glasses for nuclear waste encapsulation198227
US 4,412,861 AMethod for the recovery of uranium values from uranium tetrafluoride198328
JP S6315200 APhosphate vitrifying processing method of radioactive boric acid waste liquor—3
US 4,819,571 AProcess for the destruction of organic waste material198917
US 5,200,033 AMethod for removing organic contaminants from soils199357
US 5,246,496 APhosphate-bonded calcium aluminate cements199316
US 5,285,000 AComposition and process for organic and metal contaminant fixation in soil199434
US 5,304,710 AMethod of detoxification and stabilization of soils contaminated with chromium ore waste199481
JP H07204605 AWaste disposal material—12
US 5,457,266 AProcess for treating radioactive waste19956
US 5,541,386 APlasma arc decomposition of hazardous wastes into vitrified solids and non-hazardous gasses199689
US 5,645,518 AMethod for stabilizing low-level mixed wastes at room temperature1997114
US 5,653,872 AApparatus for removing water from aqueous sludge waste compositions199731
US 5,678,233 AMethod of immobilizing toxic or radioactive inorganic wastes and associated products199726
US 5,732,367 AReduction of leachability and solubility of radionuclides and radioactive substances in contaminated soils and materials199821
US 5,830,815 AMethod of waste stabilization via chemically bonded phosphate ceramics1998110
US 5,840,638 APhosphate glasses for radioactive, hazardous and mixed waste immobilization199826
US 5,846,894 APhosphate bonded structural products from high volume wastes199874
US 6,133,498 AMethod for producing chemically bonded phosphate ceramics and for stabilizing contaminants encapsulated therein utilizing reducing agents200096
US 6,153,809 APolymer coating for immobilizing soluble ions in a phosphate ceramic product200046
US 6,204,214 B1Pumpable/injectable phosphate-bonded ceramics200165
US 6,258,994 B1Methods of vitrifying waste with low melting high lithia glass compositions200138
US 6,283,908 B1Vitrification of waste with conitnuous filling and sequential melting200124
US 2002009622 A1Sprayable phosphate cementitious coatings and a method and apparatus for the production thereof—175
JP 2002131481 AMethod of solidification of radioactive waste—6
US 6,498,119 B2Chemically bonded phosphate ceramics of trivalent oxides of iron and manganese200223
US 6,518,212 B1Chemically bonded phospho-silicate ceramics200352

Non-Patent Literature (5)

  • Amendment dated May 4, 2007, U.S. Appl. No. 10/782,278, 8 pages.
  • Amendment dated Nov. 18, 2006, U.S. Appl. No. 10/782,278, 13 pages.
  • Bothe V. et al., "Low temperature synthesis of AIPO," Ceram. Trans., 1991, 16:689-699.
  • Gonzalez F. et al, "Reaction of orthophosphoric acid with several forms of aluminum oxide," 1980, vol. 59, No. 7 pp. 727-738.
  • Notice of Allowance dated Oct. 4, 2007, U.S. Appl. No. 10/782,278, 8 pages.