US 6,759,255 B2#9554090 Most CitedExpiredUnited States (USPTO)Utility

Method and system for detecting metal contamination on a semiconductor wafer

11Forward Citations (#9554090 Global)
0.5/yrCitation Velocity (#15401281 Global)
1.88Citation PageRank (#16003284 Global)
32Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method to detect metal contamination on a semiconductor topography is provided. The semiconductor topography may include a semiconductor substrate or a dielectric material disposed upon a semiconductor substrate. The metal contamination may be driven into the semiconductor substrate by an annealing process. Alternatively, the annealing process may drive the metal contamination into the dielectric material. Subsequent to the annealing process, a charge may be deposited upon an upper surface of the semiconductor topography. An electrical property of the semiconductor topography may be measured. A characteristic of at least one type of metal contamination may be determined as a function of the electrical property of the semiconductor topography. The method may be used to determine a characteristic of one or more types of metal contamination on a portion of the semiconductor topography or the entire semiconductor topography. A system configured to detect metal contamination on a semiconductor topography is also provided. An oven may be incorporated into the system and may be used to anneal the semiconductor topography. The system may also include a device that may be configured to de

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 11.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for detecting metal contamination in a dielectric material disposed upon a semiconductor substrate, comprising: annealing the semiconductor substrate, wherein annealing the semiconductor substrate is effective to drive the metal contamination into the dielectric material; subsequent to said annealing, measuring a tunneling voltage of the dielectric material; and determining a characteristic of the metal contamination in the dielectric material as a function of the measured tunneling voltage.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the annealed dielectric material is substantially free of damage.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein annealing the semiconductor substrate comprise heating the semiconductor substrate to an annealing temperature, and wherein the metal contamination com

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
US 3,495,269 AElectrographic recording method and apparatus with inert gaseous discharge ionization and acceleration gaps197075
US 3,496,352 ASelf-cleaning corona generating apparatus197094
US 4,599,558 APhotovoltaic imaging for large area semiconductors1986108
US 4,734,721 AElectrostatic printer utilizing dehumidified air198875
US 4,812,756 AContactless technique for semicondutor wafer testing1989216
US 5,485,091 AContactless electrical thin oxide measurements1996133
US 5,594,247 AApparatus and method for depositing charge on a semiconductor wafer199795
US 5,644,223 AUniform density charge deposit source199759
US 5,650,731 APhotovoltaic oxide charge measurement probe technique199747
US 5,661,408 AReal-time in-line testing of semiconductor wafers1997102
US 5,742,658 AApparatus and method for determining the elemental compositions and relative locations of particles on the surface of a semiconductor wafer199899
US 5,767,693 AMethod and apparatus for measurement of mobile charges with a corona screen gun199835
US 5,773,989 AMeasurement of the mobile ion concentration in the oxide layer of a semiconductor wafer199890
US 5,834,941 AMobile charge measurement using corona charge and ultraviolet light199832
WO 9,857,358 A1Method and apparatus for automatically generating schedules for wafer processing within a multichamber semiconductor wafer processing tool—22
US 5,852,232 AAcoustic sensor as proximity detector199857
US 5,866,806 ASystem for locating a feature of a surface199957
US 5,948,972 ADual stage instrument for scanning a specimen199985
US 5,955,661 AOptical profilometer combined with stylus probe measurement device199962

Non-Patent Literature (5)

  • "Contactless Electrical Equivalent Oxide Thickness Measurement," IBM Technical Disclosure Bulletin, vol. 29, No. 10, 1987, pp. 4622-4623.
  • "Contactless Photovoltage vs. Bias Method for Determining Flat-Band Voltage," IBM Technical Disclosure Bulletin, vol. 32, vol. 9A, 1990, pp. 14-17.
  • Cosway et al., Manufacturing Implementation of Corona Oxide Silicon (COS) Systems for Diffusion Furnace Contamination Monitoring, 1997 IEEE/SEMI Advanced Semiconductor Manufacturing Conference and Workshop ASMC 97 Proceedings, Cambridge, MA, USA, Sep. 10-12.*
  • Miller, "A New Approach for Measuring Oxide Thickness," Semiconductor International, Jul. 1995, pp. 147-148.
  • Numerical Recipies in C, The Art of Scientific Computing, 2nd Ed., (C) Cambridge University Press 1988, 1992, p. 683.