Contactless electrical thin oxide measurements
Abstract
A method for measuring the thickness of very thin oxide layers on a silicon substrate. A corona discharge source repetitively deposits a calibrated fixed charge density on the surface of the oxide. The resultant change in oxide surface potential for each charge deposition is measured. By choosing a starting value for an assumed oxide thickness, the approximate change in silicon bandbending per corona discharge step is determined. The cumulative changes in bandbending versus oxide surface potential yields an experimental bandbending versus bias characteristic. A theoretical bandbending versus bias characteristic is established. The experimental and theoretical characteristics are matched at predetermined points thereof and then the assumed oxide thickness is iterated until both characteristics superimpose in the silicon accumulation region. The iterated oxide thickness that allows both characteristics to superimpose is the oxide thickness value being sought. The finally evolved experimental characteristic also is used to determine the interface states density of the oxide. Specially designed corona discharge guns are described for use with the oxide thickness and interface states de
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 133.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In a method for measuring the thickness of an insulating layer on a semiconductor substrate, the steps comprising: repetitively depositing a fixed charge density on the surface of said layer, measuring the resultant changes in the surface potential of said layer relative to the bulk of said substrate, establishing a theoretical bandbending versus bias characteristic for said layer and substrate, undergoing said repetitive deposition of charge density, for an assumed value of said thickness, determining an experimental bandbending versus bias characteristic using said measured change in t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 133 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (5)
- M. S. Fung, et al, "Contactless Photovoltage vs Bias Method for Determining Flat-Band Voltage" IBM Technical Disclosure Bulletin, V. 32, No. 9A, pp. 14-17, Feb. 1990.
- M. S. Fung, et al, Contactless Photovoltage vs Bias Method for Determining Flat Band Voltage IBM Technical Disclosure Bulletin, V. 32, No. 9A, pp. 14 17, Feb. 1990.
- R. Hamers, et al, "High Spatial Resolution Measurement of Doping, Band-Bending, and Recombination at Semiconductor Surfaces" IBM Technical Disclosure Bulletin, V. 33, No. 1B, pp. 91-92, Jun. 1990.
- R. Hamers, et al, High Spatial Resolution Measurement of Doping, Band Bending, and Recombination at Semiconductor Surfaces IBM Technical Disclosure Bulletin, V. 33, No. 1B, pp. 91 92, Jun. 1990.
- R. L. Verkuil, "Rapid Contactless Method for Measuring Fixed Oxide Charge Associated with Silicon Processing" IBM Technical Disclosure Bulletin, V. 24, No. 6, pp. 3048-3053, Nov. 1981.