Patents
US 6,734,050 B2#16175945 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing a crystalline semiconductor film

7Forward Citations (#16175945 Global)
0.3/yrCitation Velocity (#24973407 Global)
1.23Citation PageRank (#30818193 Global)
5Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A spin addition method for catalyst elements is simple and very important technique, because the minimum amount of a catalyst element necessary for crystallization can be easily added by controlling the catalyst element concentration within a catalyst element solution, but there is a problem in that uniformity in the amount of added catalyst element within a substrate is poor. The non-uniformity in the amount of added catalyst element within the substrate is thought to influence fluctuation in crystallinity of a crystalline semiconductor film that has undergone thermal crystallization, and exert a bad influence on the electrical characteristics of TFTs finally structured by the crystalline semiconductor film. The present invention solves this problem with the aforementioned conventional technique. If the spin rotational acceleration speed is set low during a period moving from a dripping of the catalyst element solution process to a high velocity spin drying process in a catalyst element spin addition step, then it becomes clear that the non-uniformity of the amount of added catalyst element within the substrate is improved. The above stated problems are therefore solved by applyin

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 7.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a crystalline semiconductor film containing silicon, said method comprising: a first step of depositing an amorphous semiconductor film containing silicon over an insulating substrate; a second step of adding a metallic element for promoting crystallization to a entire surface of the amorphous semiconductor film by a spin addition method; and a third step of forming the crystalline semiconductor film by heat treating the amorphous semiconductor film; wherein a rotational acceleration speed in the spin addition method is from 5 to 120 rpm/sec.

  2. Claim 2Depends on #1

    A method of manufacturing a crystalline semiconductor film according to claim 1 , wherein the insulating substrate has a square shape.

  3. Claim 3Independent Claim

    A method of manufacturing a crystalline semiconductor film according

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗