Patents
US 7,960,296 B2#64704165 Most CitedActiveUnited States (USPTO)Utility

Crystalline semiconductor film, method of manufacturing the same, and semiconductor device

0Forward Citations (#64704165 Global)
0.0/yrCitation Velocity (#64704165 Global)
0.56Citation PageRank (#64704165 Global)
40Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A spin addition method for catalyst elements is simple and very important technique, because the minimum amount of a catalyst element necessary for crystallization can be easily added by controlling the catalyst element concentration within a catalyst element solution, but there is a problem in that uniformity in the amount of added catalyst element within a substrate is poor. The non-uniformity in the amount of added catalyst element within the substrate is thought to influence fluctuation in crystallinity of a crystalline semiconductor film that has undergone thermal crystallization, and exert a bad influence on the electrical characteristics of TFTs finally structured by the crystalline semiconductor film. The present invention solves this problem with the aforementioned conventional technique. If the spin rotational acceleration speed is set low during a period moving from a dripping of the catalyst element solution process to a high velocity spin drying process in a catalyst element spin addition step, then it becomes clear that the non-uniformity of the amount of added catalyst element within the substrate is improved. The above stated problems are therefore solved by applyin

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 40 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a crystalline semiconductor film containing silicon, said method comprising: a first step of depositing an amorphous semiconductor film containing silicon over an insulating substrate; a second step of adding a metallic element for promoting crystallization to an entire surface of the amorphous semiconductor film by a spin addition method; and a third step of forming the crystalline semiconductor film by heat treating the amorphous semiconductor film; wherein a rotational acceleration speed y in the spin addition method satisfies y≦Ax −B (where x is a diagonal dimens

  2. Claim 2Depends on #1

    A method of manufacturing a crystalline semiconductor film according to claim 1 , wherein the insulating substrate has a square shape.

  3. Claim 3Independent Claim

    A method of manufacturing a crystalline semico

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (40)

PatentTitleYearCitations
US 5,403,762 AMethod of fabricating a TFT1995178
US 5,403,772 AMethod for manufacturing semiconductor device1995596
JP H07183538 ASemiconductor device and manufacture thereof—11
JP H07211636 AMethod and apparatus for producing semiconductor device—11
US 5,563,426 AThin film transistor1996301
US 5,572,046 ASemiconductor device having at least two thin film transistors1996108
US 5,604,360 ASemiconductor device including a plurality of thin film transistors at least some of which have a crystalline silicon film crystal-grown substantially in parallel to the surface of a substrate for the transistor1997293
US 5,643,826 AMethod for manufacturing a semiconductor device19971,815
US 5,654,203 AMethod for manufacturing a thin film transistor using catalyst elements to promote crystallization1997152
US 5,693,541 AMethod for manufacturing a semiconductor device using a silicon nitride mask199771
US 5,700,333 AThin-film photoelectric conversion device and a method of manufacturing the same1997183
US 5,712,191 AMethod for producing semiconductor device1998198
US 5,728,626 ASpin-on conductor process for integrated circuits199856
US 5,804,473 AThin film semiconductor device having a polycrystal active region and a fabrication process thereof199842
US 5,843,833 AMethod for producing semiconductor device199880
US 5,843,225 AProcess for fabricating semiconductor and process for fabricating semiconductor device1998126
US 5,888,857 ASemiconductor device and method for manufacturing the same1999104
US 5,916,717 AProcess utilizing relationship between reflectivity and resist thickness for inhibition of side effect caused by halftone phase shift masks199923
US 5,994,164 ANanostructure tailoring of material properties using controlled crystallization1999190
US 5,994,172 AMethod for producing semiconductor device199939
US 6,013,544 AMethod for fabricating a semiconductor device200068
US 6,074,901 AProcess for crystallizing an amorphous silicon film and apparatus for fabricating the same200029
US 6,140,165 ASemiconductor device forming method200059
JP 2001135574 AMethod of fabrication for semiconductor device—7
US 6,241,817 B1Method for crystallizing amorphous layer200151
US 6,323,071 B1Method for forming a semiconductor device200148
US 6,338,991 B1Semiconductor device and method for manufacturing the same200262
US 6,348,367 B1Method for manufacturing a semiconductor device200231
US 6,413,805 B1Semiconductor device forming method200233
US 6,465,287 B1Method for fabricating a semiconductor device using a metal catalyst and high temperature crystallization200267

Non-Patent Literature (5)

  • Dausch et al., "Antiferroelectric/ferroelectric composite thin films," Applications of Ferroelectrics, 1994, ISAF '94, Proceedings of the Ninth IEEE International Symposium, Aug. 7-10, 1994, pp. 701-704.
  • Ito et al., "The performances of the novel nozzle-scan coating method," Microprocesses and Nanotechnology Conference, 2000 International, Jul. 11-13, 2000, pp. 298-299.
  • Kakkad et al., "Crystallized Si films by low-temperature rapid thermal annealing of amorphous silicon," J. Appl. Phys. 65, No. 5, Mar. 1, 1989, pp. 2069-2072.
  • Schwartz et al., "Electrical properties of chemically derived (Pb, La) TiO3 thin films," ISAF'91 Proceedings of the 7th IEEE International Symposium on Applications of Ferroelectrics, 1990, IEEE 7th International Symposium, Jun. 6-8, 1990, pp. 254-257.
  • T. Kitano, "Novel coating apparatus using nozzle-scan technique," Semiconductor Manufacturing, 2000, Proceedings of ISSM 2000, The Ninth International Symposium on Semiconductor Manufacturing, Sep. 26-28, 2000, pp. 395-398.