Patents
US 6,727,176 B2#4320587 Most CitedExpiredUnited States (USPTO)Utility

Method of forming reliable Cu interconnects

20Forward Citations (#4320587 Global)
0.9/yrCitation Velocity (#7858761 Global)
2.43Citation PageRank (#10666335 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Reliable Cu interconnects are formed by filling an opening in a dielectric layer with Cu and then laser thermal annealing in NH 3 to reduce copper oxide and to reflow the deposited Cu, thereby eliminating voids and reducing contact resistance. Embodiments include laser thermal annealing employing an NH 3 flow rate of about 200 to about 2,000 sccn.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 20.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device, the method comprising: forming an opening in a dielectric layer; depositing copper (Cu) or a Cu alloy to fill the opening; and laser thermal annealing the deposited Cu or Cu alloy in ammonia (NH 3 ) to reflow the deposited Cu or Cu alloy.

  2. Claim 2Depends on #1

    The method according to claim 1 , comprising laser thermal annealing by impinging a pulsed laser light beam on the deposited Cu or Cu alloy at a radiant fluence of about 0.28 to about 0.34 joules/cm 2 .

  3. Claim 3Depends on #2

    The method according to claim 2 , comprising laser thermal annealing to heat the deposited Cu or Cu alloy to a temperature of about 983° C. to about 1183° C., thereby reflowing the deposited Cu or Cu alloy.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗