Patents
US 6,153,522 A#1465426 Most CitedExpiredUnited States (USPTO)Utility

Semiconductor device manufacturing method

39Forward Citations (#1465426 Global)
1.5/yrCitation Velocity (#3402920 Global)
5.32Citation PageRank (#2996912 Global)
3Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A semiconductor device manufacturing method of the present invention comprises the steps of forming a groove on an insulating film formed over a semiconductor substrate, forming a first copper film on the insulating film and in the groove by sputtering using a target, reflowing the first copper film by heating it, growing a second copper film on the first copper film by plating or chemical vapor deposition, and removing the second copper film and the first copper film on the insulating film by chemical mechanical polishing to remain at least the first copper film in the groove. Accordingly, in the semiconductor device manufacturing method to provide copper wirings, increase in resistance can be suppressed by firmly embedding copper into the groove and also electromigration resistance of copper wirings can be improved.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 39.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising the steps of: forming a groove in an insulating film formed over a semiconductor substrate; forming a first copper film on the insulating film and in the groove by sputtering using a target; reflowing the first copper film by heating it; forming a second copper film on the first copper film by plating or chemical vapor deposition; and removing the second copper film and the first copper film on the insulating film by chemical mechanical polishing to remain at least the first copper film in the groove.

  2. Claim 2Depends on #1

    A method of manufacturing a semiconductor device according to claim 1, wherein the step of reflowing the first copper film is executed at a substrate temperature of 350° C. to 450° C.

  3. Claim 3Independent Claim

    A method of manufacturing a semiconductor device accordi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗