Patents
US 6,699,337 B2#3571933 Most CitedExpiredUnited States (USPTO)Utility

Copper-base alloys having improved punching properties on press and a process for producing them

22Forward Citations (#3571933 Global)
1.0/yrCitation Velocity (#6184070 Global)
6.63Citation PageRank (#2094767 Global)
12Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An ingot of a copper-base alloy containing a total of 0.01-30 wt % of at least one element selected from among Sn, Ni, P, Zn, Si, Fe, Co, Mg, Ti, Cr, Zr and Al, with the balance being Cu and incidental impurities, is homogenized by annealing, subjected to repeated cycles of cold rolling and annealing, then cold rolled at a reduction ratio Z which satisfies the following relation:[where Z is the percent reduction by cold rolling; X is the content in wt % of Sn; Y is the total content in wt % of any elements other than Sn], and thereafter subjected to cold annealing at a temperature below the recrystallization temperature to produce a copper-base alloy having a surface X-ray diffraction intensity ratio SND of at least 10 [SND=I{220}/I{200}; I{220} is the X-ray diffraction intensity of {220} and I{200} is the X-ray diffraction intensity of {200}] while exhibiting improved punching properties on press due to the balance between electrical conductivity, strength, spring property, hardness and bending properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 22.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A copper-base alloy having improved punching properties on press that contains a total of 0.01-30 wt % of at least one element selected from the group consisting of Sn, Ni, P, Zn, Si, Fe, Co, Mg, Ti, Cr, Zr and Al, with the balance being Cu and incidental impurities, and which has a surface X-ray diffraction intensity ratio S D of at least 10 [S ND =I{220}/I{200}; I{220} is the X-ray diffraction intensity of {220} and I{200} is the X-ray diffraction intensity of {200}].

  2. Claim 2Independent Claim

    A copper-base alloy having improved punching properties on press that contains a total of 0.01-30 wt % of at least one element selected from the group consisting of Sn, Ni, P, Zn, Si, Fe, Co, Mg, Ti, Cr, Zr and Al, with the balance being Cu and incidental impurities, and which has a surface X-ray diffraction intensity ratio S ND of at least 10 [S ND =(I{220}+I

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗