Patents
US 5,322,575 A#1831975 Most CitedExpiredUnited States (USPTO)Utility

Process for production of copper base alloys and terminals using the same

34Forward Citations (#1831975 Global)
1.1/yrCitation Velocity (#6026019 Global)
6.21Citation PageRank (#2328535 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A copper base alloy for terminals that is superior in all aspects of tensile strength, spring limits, conductivity, and stress relaxation characteristics can be produced by a process repeating the cycles consisting of hot-rolling, cold-rolling and annealing, in which process an ingot is prepared by melting and casting an alloy containing 1.0-3.0 wt % Ni, 0.02-0.15 wt % P. 0.5-2.0 wt. % Sn and, as an optional component, 0.01-2.0 wt % Zn, with the balance being Cu and incidental impurities, and with the ratio of weight percentages of Ni to P being within the range of 10-50%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 34.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a copper alloy for terminals from an ingot of a copper alloy to obtain a sheet of a desired final thickness comprising (a) preparing the ingot by melting and casting an alloy consisting essentially, on a weight basis, of 1.0-3.0% Ni, 0.02-0.15% P and 0.5-2.0% Sn, with the balance being Cu and incidental impurities, and with a ratio of weight percentages of Ni to P (Ni/P) being 10-50, (b) hot rolling and (c) repeating cycles of cold-rolling and annealing, wherein prior to a first cold-rolling step after the hot-rolling, cooling from a temperature of not less than 700

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗