The invention relates to methods of vitrifying waste and for lowering the melting point of glass forming systems by including lithia formers in the glass forming composition in significant amounts, typically from about 0.16 wt % to about 11 wt %, based on the total glass forming oxides. The lithia is typically included as a replacement for alkali oxide glass formers that would normally be present in a particular glass forming system. Replacement can occur on a mole percent or weight percent basis, and typically results in a composition wherein lithia forms about 10 wt % to about 100 wt % of the alkali oxide glass formers present in the composition. The present invention also relates to the high lithia glass compositions formed by these methods. The invention is useful for stabilization of numerous types of waste materials, including aqueous waste uranium oxides The decrease in melting point achieved by the present invention desirably prevents volatilization of hazardous or radioactive species during vitrification.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 3.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An alkali oxide-lime-silica glass suitable for immobilizing radioactive, hazardous, or mixed waste, consisting essentially of: (a) SiO 2 in an amount ranging from about 46 wt % to about 66 wt %; (b) CaO in an amount ranging from about 5 wt % to about 28 wt %; (c) Na 2 O in an amount ranging from about 1.9 wt % to about 25 wt %; (d) Li 2 O in an amount ranging from about 3 wt % to about 11 wt %; and (e) a uranium oxide selected from the group consisting of U 3 O 8 in the range from about 0.5 wt % to about 12 wt % and UO 2 in an amount ranging from about 0.4 wt % to about 12 wt %.

  2. Claim 2Depends on #1

    The alkali oxide-lime-silica glass composition according to claim 1 including: (f) Al 2 O 3 in an amount ranging from about 2.5 wt % to about 18 wt %.

  3. Claim 3Independent Claim

    The alkali oxide-li

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 2,859,138 AComposition and method for coating a ceramic body195821
US 3,265,627 AAddition of lithium values in conversion of fission-product wastes to a glass-like solid for disposal196611
US 3,876,481 AGlass compositions, fibers and methods of making same197568
DE 2,534,014 A1Thermodynamisch stabiles glaskeramikprodukt oder glaskeramikaehnliches produkt zur endgueltigen beseitigung hochradioaktiver abfaelle—8
US 4,020,004 AConversion of radioactive ferrocyanide compounds to immobile glasses197716
US 4,097,401 AThermodynamically stable product for permanent storage and disposal of highly radioactive liquid wastes197828
US 4,147,835 AArticle having self-cleaning coating197946
US 4,182,437 AUnstable devitrifiable glasses and friction materials containing them198069
EP 0,071,927 A1Process for solidifying radioactive wastes—8
GB 2,106,891 AOptical and opthalmic glass—18
US 4,464,294 AProcess for the stabilization of radioactive wastes198425
US 4,514,329 AProcess for vitrifying liquid radioactive waste198556
US 4,725,383 AProcess for volume reduction and solidification of a radioactive sodium borate waste solution198821
US 4,759,879 AGlass former composition and method for immobilizing nuclear waste using the same198821
US 4,772,431 AProcess for the immobilization of nuclear waste in a borosilicate glass198824
EP 0,287,345 A1Glass composition for and method for preparation of gradient index lens—30
US 4,797,232 AProcess for the preparation of a borosilicate glass containing nuclear waste198935
US 4,820,325 ATreatment of toxicant-impregnated filter cake198912
US 5,102,439 AMethod for melting glass by measurement of non-bridging oxygen199218
GB 2,263,478 ALead-and and cadmium-free glass composition for glazing, enameling and decorating—22
US 5,292,375 ARemoval of lead based coating by vitrification199412
US 5,403,664 AMarble-like glass ceramic199525
US 5,530,174 AMethod of vitrifying high-level radioactive liquid waste199616
US 5,616,160 AProcess for vitrifying incinerator ash199722

Non-Patent Literature (5)

  • Copy of International Search Report issued in PCT/US99/09425 on Dec. 16, 1999.
  • Database WPI, Section Ch. Week 199705, Derwent Publications Ltd., London, GB, Class E36, AN 1997-050200 (Russian Publication No. 2 059 579) to Mash Wks Khrunichev, May 10, 1996.
  • Database WPI, Section Ch. Week 8846, Derwent Publications Ltd., London, GB; Class K07, AN 88-327039 (JP 63 241400 to New ajapan Radio Co. Ltd.).
  • Donald, I.W. et al., "Review. The Immobilization of High Level Radioactive Wastes Using Ceramics and Glasses," J. Materials Science, vol. 32, No. 22 Nov. 15, 1997, p. 37.
  • Hara, M., "Ion-Channel Match in Mixed Alkali Glasses," J. Non-Cryst. Solids, vols. 131-133, p. 1076 (1991).