Thermodynamically stable product for permanent storage and disposal of highly radioactive liquid wastes
Abstract
Highly radioactive liquid wastes are permanently stored in a solidification matrix containing the components of a known borosilicate glass together with nucleation agents selected from the group consisting of oxides of Li, K, Mg, Mo and Cr, fluorides of those metals and of Al, and pure noble metals in the elemental form with particles with sizes smaller than 0.1 mu m in diameter, and up to 35% by weight of waste fission and corrosion products or waste fission and corrosion products and gadolinium oxide. The product is produced by denitrating and calcining the radioactive waste solution, melting the calcined waste product together with a borosilicate frit containing nucleation agents at a temperature of between 1,050 DEG and 1,200 DEG C, and maintaining it in its melted state for 3 to 5 hours, subsequently cooling the resulting mixture until to a given temperature and maintaining it at this temperature for a given time period to permit nucleation to occur, then elevating the temperature of the mixture with an constant heating rate until to a given higher temperature, maintaining it at this higher temperature for about 24 hours, and finally cooling it with a constant cooling rate to
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 28.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A thermodynamically stable microcrystalline glass ceramic or glass ceramic-like product for permanent disposal and storage of highly radioactive wastes in a manner harmless to the environment or the biocycle, comprising: (a) a solidifying matrix containing the components of a borosilicate glass including, by weight of the thermodynamically stable product, 35 to 50% SiO 2 , 3 to 6% TiO 2 , 5 to 10% Al 2 O 3 , 3 to 6% B 2 O 3 , 0 to 5% Na 2 O; (b) a plurality of nucleation agents, including, by weight, 3 to 6% MgO, 8 to 10% Li 2 O and 3 to 6% K 2 O; and (c) 20 to 30% by weight of waste
- Claim 2Depends on #1
A product as defined in claim 1, which contains at least one further nucleation a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 28 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (5)
- Bonniaud et al., "Fission Product Retention in Glasses and Micas", Geneva II, 1958, vol. 18, pp. 33-36 (especially pp. 34-36).
- Chem. Abstracts, vol. 75, #121136f, "Parametric Study . . . Waste Solidification", 1971.
- Chem. Abstracts. vol. 77, #171622y.
- Goldman et al., "Retention of Fission Products . . . Fusions", Geneva II, 1958, vol. 18, pp. 27-32.
- Heine et al., "Research on Glasses . . . Fixation", HMI-B 109 (1971) as abstracted in Chem. Abstracts, vol. 82, #159948e.