US 6,610,583 B2#28778017 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing semiconductor thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured

3Forward Citations (#28778017 Global)
0.1/yrCitation Velocity (#41126236 Global)
1.42Citation PageRank (#24845060 Global)
3Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing a semiconductor thin film having high carrier mobility, and a magnetoelectric conversion element provided with the semiconductor thin film manufactured by the aforementioned method are provided. The temperature of the Si single crystal substrate is raised to 270° C. to 320° C., and an In buffer layer is formed by an electron beam heating type vacuum evaporation method. Subsequently, an initial seed layer made of Sb and In is formed. The temperature of the Si single crystal substrate is raised to 460° C. to 480° C., and thereafter, a retention time approximated by a predetermined function of the temperature of the Si single crystal substrate is provided. Then, a main growth layer made of Sb and In is formed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor thin film, comprising the steps of: (a) removing a surface oxide film from a substrate having a surface comprising a silicon single crystal; (b) hydrogen terminating the surface of said substrate; (c) forming a buffer layer comprising indium on said substrate; (d) forming an initial seed layer comprising indium and antimony on said buffer layer; and (e) forming a main growth layer comprising indium and antimony on said initial seed layer while a temperature of said substrate is kept at 465° C. to 475° C.

  2. Claim 2Depends on #1

    A method for manufacturing a semiconductor thin film according to claim 1 , wherein steps (a) and (b) are performed using an aqueous solution selected from the group consisting of an aqueous solution of hydrogen fluoride, an aqueous solutio

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Bunshah, "Deposition Technologies for Films and Coatings," Chapter 4, p. 102, Noyes Publications, New York, 1982.