A method of fabricating a semiconductor thin film is initiated with preparing a substrate having a surface consisting of a single crystal of Si. The surface has an oxide film. Then, the oxide film is removed. The dangling bonds of the Si atoms on the surface are terminated with hydrogen atoms. An initial layer is formed on the substrate of the single crystal of Si terminated with the hydrogen atoms, of at least one selected from the group consisting of Al, Ga, and In. A buffer layer containing at least In and Sb is formed on the initial layer. A semiconductor thin film containing at least In and Sb is formed on the buffer layer at a temperature higher than the temperature at which the buffer layer is started to be formed. There is also disclosed a method of fabricating a Hall-effect device. This method is initiated with forming a semiconductor thin film by making use of the above-described fabrication method. Then, electrodes are attached to the thin film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating a semiconductor thin film, comprising the steps of: preparing a substrate having a surface including a single crystal of Si; removing an oxide film from the surface of the substrate and terminating dangling bonds of Si atoms on the surface with hydrogen atoms; forming an initial layer of at least one member selected from the group consisting of Al, Ga, and In on the substrate terminated with the hydrogen atoms; forming a buffer layer containing at least In and Sb on the initial layer; and forming a semiconductor thin film containing at least In and Sb on said bu

  2. Claim 2Depends on #1

    The method in accordance with claim 1, wherein (A) said initial layer is formed of Al to a thickness of 0.1 to 3 nm; (B) said buff

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (13 of 13 total)

PatentTitleYearCitations
US 2003203601 A1Method for manufacturing semiconductor thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured—0
US 2006205189 A1Manufacturable recessed strained RSD structure and process for advanced CMOS—15
US 2006024934 A1Chemical treatment to retard diffusion in a semiconductor overlayer—6
US 2007042572 A1Deposition of silicon germanium on silicon-on-insulator structures and bulk substrates—10
US 6,630,882 B1Composite magnetic sensor200329
US 2005026400 A1Methods for depositing amorphous materials and using them as templates for epitaxial films by solid phase epitaxy—15
US 7,446,005 B2Manufacturable recessed strained RSD structure and process for advanced CMOS20084
US 6,610,583 B2Method for manufacturing semiconductor thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured20033
US 2005029608 A1Method for manufacturing semiconductor thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured—4
US 6,893,946 B2Method for manufacturing semiconductor thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured20051
EP 1,168,466 A3Method for manufacturing semiconductors thin film, and magnetoelectric conversion element provided with semiconductor thin film thereby manufactured—0
US 7,071,103 B2Chemical treatment to retard diffusion in a semiconductor overlayer20062
US 7,029,995 B2Methods for depositing amorphous materials and using them as templates for epitaxial films by solid phase epitaxy200613

Non-Patent Literature (4)

  • Chyi et al., "Molecular Beam Epitaxial Growth and Characterization of InSb on Si," Applied Physics Letters, vol. 54, No. 11, Mar. 13, 1989, pp. 1016-1018.
  • Chyi et al., Molecular Beam Epitaxial Growth and Characterization of InSb on Si, Applied Physics Letters, vol. 54, No. 11, Mar. 13, 1989, pp. 1016 1018.
  • Konno et al., "New InSb and GaAs Fabrication Techniques Yield Better, Cheaper Hall Element," Journal of Electronic Engineering, Oct., 1975, vol. 107, pp. 24-28.
  • Konno et al., New InSb and GaAs Fabrication Techniques Yield Better, Cheaper Hall Element, Journal of Electronic Engineering, Oct., 1975, vol. 107, pp. 24 28.