Abstract

A method for coating a nickel- or cobalt-based superalloy surface by slurry deposition/heat diffusion. The method includes preparing a slurry of a metal coating powder mixed into an adhesive carrier that will burn off ash-free during a diffusion cycle, depositing the slurry onto the surface of a Ni- or Co-based superalloy material to form a coated surface, and heating the coated surface to a temperature of at least about 1600° F. to diffuse the metal coating powder into the metal substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 12.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of coating a superalloy surface, said method comprising: (1) preparing a slurry comprising a metal coating powder and a carrier/adhesive resin that vaporizes leaving essentially no contaminating residue when heated to a temperature effective to diffuse the metal coating powder into the surface of a superalloy material; wherein said carrier/adhesive resin is a urethane oligomer/(meth) acrylate monomer blend that vaporizes leaving no contaminating residue when heated to a temperature of about 1250° F.; (2) depositing said slurry onto the surface of a superalloy material to form a coated

  2. Claim 2Depends on #1

    The method of claim 1 wherein said metal coating powder comprises an aluminum