Patents
US 9,624,583 B2#100491488 Most CitedActiveUnited States (USPTO)Utility

Slurry-based coating techniques for smoothing surface imperfections

0Forward Citations (#100491488 Global)
0.0/yrCitation Velocity (#100491488 Global)
0.56Citation PageRank (#100491488 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An article may include a substrate defining a surface imperfection and a coating deposited over the substrate. The coating does not substantially reproduce the surface imperfection, and the coating comprises mullite and at least one rare earth silicate, rare earth oxide, alumina, boron oxide, alkali metal oxide, alkali earth metal oxide, silicon, barium strontium aluminosilicate, barium aluminosilicate, strontium aluminosilicate, calcium aluminosilicate, magnesium aluminosilicate, or lithium aluminosilicate. In some examples, the coating may be a first coating deposited from a slurry over the substrate, and a second coating may be deposited over the first coating. In other examples, a first coating that substantially reproduces the surface imperfection may be deposited over the substrate, and the coating that does not substantially reproduce the surface imperfection may be deposited over the first coating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method comprising: depositing a first coating over at least a portion of a substrate, wherein the substrate comprises at least one of a superalloy, a ceramic, or a ceramic matrix composite, wherein the substrate defines a surface imperfection, and wherein a surface of the first coating opposite the substrate substantially reproduces the surface imperfection; depositing from a slurry a second coating over at least a portion of the surface of the first coating, wherein, upon deposition of the second coating, a surface of the second coating opposite the first coating does not substantially repr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,859,061 ACorrosion resistant coating system for ferrous metal articles having brazed joints197524
US 3,962,059 AProcess and device for electrophoretically plating metal parts197624
US 4,031,274 AMethod for coating cavities with metal197737
US 4,132,816 AGas phase deposition of aluminum using a complex aluminum halide of an alkali metal or an alkaline earth metal as an activator197983
US 4,148,275 AApparatus for gas phase deposition of coatings197990
US 4,347,267 ADiffusion coating through restrictions198249
US 4,358,480 AMethod of repairing surface damage to porous refractory substrates198222
US 4,501,766 AFilm depositing apparatus and a film depositing method198549
US 4,965,095 AMethod for refurbishing used jet engine hot section airfoils199053
US 5,041,309 AMethod of chromizing a workpiece by applying a coating containing chromium particles onto a ceramic carrier, positioning the carrier proximate the workpiece, and heating both carrier and workpiece to diffuse chromium particles into the workpiece199131
US 5,057,196 AMethod of forming platinum-silicon-enriched diffused aluminide coating on a superalloy substrate199155
US 5,071,678 AProcess for applying gas phase diffusion aluminide coatings199181
US 5,217,757 AMethod for applying aluminide coatings to superalloys199358
US 5,334,417 AMethod for forming a pack cementation coating on a metal surface by a coating tape199458
US 5,355,668 ACatalyst-bearing component of gas turbine engine199463
US 5,366,754 AReduced fat peanut butter product and method of making199442
US 5,366,765 AAqueous slurry coating system for aluminide coatings199498
US 5,683,825 AThermal barrier coating resistant to erosion and impact by particulate matter1997196
US 5,807,428 ASlurry coating system199831
US 5,824,366 ASlurry coating system199840
US 5,958,204 AEnhancement of coating uniformity by alumina doping199925
US 5,976,337 AMethod for electrophoretic deposition of brazing material199945
US 5,997,604 ACoating tape199927
US 6,045,863 ALow activity localized aluminide coating200034
EP 1,010,774 A1Article with hafnium-silicon-modified platinum-aluminium bond or environmental coating—30
US 6,110,262 ASlurry compositions for diffusion coatings200072
WO 0,105,579 A2One-step noble metal-aluminide coatings—6
US 6,180,170 B1Device and method for preparing and/or coating the surfaces of hollow construction elements200130
EP 1,088,908 A2A method for smoothing the surface of a protective coating—62
US 6,235,352 B1Method of repairing a thermal barrier coating200139

Non-Patent Literature (5)

  • Chen, "Slurry development for the deposition of a GdSiO4+Mullite environmental barrier coating on silicon carbide," Journal of Ceramic Processing Research, vol. 8, No. 2, pp. 142-144, 2007.
  • European Office Action from counterpart European application No. 10 158 950.5-1362, dated Oct. 23, 2013, 3 pp.
  • Extended European Search Report from European application No. 10158950.5, dated Jun. 14, 2010, 13 pp.
  • Final Office Action for U.S. Appl. No. 11/963,249, dated Dec. 12, 2011, 21 pages.
  • Final Office Action from U.S. Appl. No. 14/213,466, dated Mar. 4, 2016, 8 pp.