Abstract
An embodiment of the present invention is a method of forming an ultra-thin dielectric layer, the method comprising the steps of: providing a substrate having a semiconductor surface; forming an oxygen-containing layer on the semiconductor surface; exposing the oxygen-containing layer to a nitrogen-containing plasma to create a uniform nitrogen distribution throughout the oxygen-containing layer; and re-oxidizing and annealing the layer to stabilize the nitrogen distribution, heal plasma-induced damage, and reduce interfacial defect density.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 47.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for forming an integrated circuit structure, comprising the steps of: providing a substrate having a semiconductor surface; forming an oxygen-containing layer on said semiconductor surface; exposing said oxygen-containing layer to a nitrogen plasma to create a uniform nitrogen distribution throughout said oxygen-containing layer; and re-oxidizing a resulting nitrided layer by consecutive anneal steps in a mixture of H2 and N2, and then a mixture of O2 and N2 for healing plasma-induced damage and reducing interfacial defect density.
- Claim 2Depends on #1
The method according to claim 1 wherein said oxygen-containing layer is an ultra-thin silicon dioxide layer in the thickness range from 0.6 to 2.0 nm.
- Claim 3Depends on #1
The method according to claim 1 wherein said oxygen-containing layer is an oxynitride la
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗