Patents
US 7,964,514 B2#39381207 Most CitedActiveUnited States (USPTO)Utility

Multiple nitrogen plasma treatments for thin SiON dielectrics

2Forward Citations (#39381207 Global)
0.1/yrCitation Velocity (#41594483 Global)
1.03Citation PageRank (#40109582 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for the deposition of a dielectric film including forming silicon nitride on the surface of the substrate, oxidizing the silicon nitride on the surface of the substrate, exposing the surface of the substrate to a hydrogen-free nitrogen source, and annealing the substrate. A method for the deposition of a dielectric film including forming silicon nitride on the surface of the substrate, oxidizing the silicon nitride on the surface of the substrate, including exposing the surface of the substrate to a gas selected from the group of oxygen, nitric oxide, and nitrous oxide, and exposing the surface of the substrate to a hydrogen-free nitrogen source, wherein the hydrogen-free nitrogen source is a gas selected from the group of nitrogen, nitric oxide, and nitrous oxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the deposition of a dielectric film, comprising: forming silicon nitride on a surface of a substrate within a reaction chamber; oxidizing the silicon nitride on the surface of the substrate, wherein oxidizing the silicon nitride further comprises maintaining a substrate surface temperature of about 800° C. to about 1,100° C.; exposing the oxidized silicon nitride on the surface of the substrate to a hydrogen-free nitrogen precursor in a plasma, wherein the substrate is heated to a temperature within a range from about 20° C. to about 500° C. during the exposing of the oxidized sil

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,725,560 ASilicon oxynitride storage node dielectric198842
US 5,198,392 AMethod of forming a nitrided silicon dioxide (SiOx Ny) film199333
JP H06140392 AManufacture of semiconductor device—19
US 5,536,681 APE-OX/ozone-TEOS gap filling capability by selective N2 treatment on PE-OX199642
US 5,591,494 ADeposition of silicon nitrides by plasma-enhanced chemical vapor deposition199796
US 5,731,238 AIntegrated circuit having a jet vapor deposition silicon nitride film and method of making the same199845
EP 0,847,079 A2Method of manufacturing an MIS electrode—28
US 5,780,115 AMethods for fabricating electrode structures including oxygen and nitrogen plasma treatments199856
US 5,939,131 AMethods for forming capacitors including rapid thermal oxidation199930
US 6,020,243 AZirconium and/or hafnium silicon-oxynitride gate dielectric2000405
US 6,041,734 AUse of an asymmetric waveform to control ion bombardment during substrate processing200096
US 6,063,704 AProcess for incorporating silicon oxynitride DARC layer into formation of silicide polysilicon contact200045
US 6,077,737 AMethod for forming a DRAM having improved capacitor dielectric layers200035
US 6,136,688 AHigh stress oxide to eliminate BPSG/SiN cracking200016
US 6,136,654 AMethod of forming thin silicon nitride or silicon oxynitride gate dielectrics2000174
US 6,162,709 AUse of an asymmetric waveform to control ion bombardment during substrate processing200091
US 2001003661 A1Method of forming a capacitor—2
US 6,268,267 B1Silicon-oxynitride-oxide (SXO) continuity film pad to recessed bird's beak of LOCOS20019
US 6,297,162 B1Method to reduce silicon oxynitride etch rate in a silicon oxide dry etch200143
US 6,326,657 B1Semiconductor device having both memory and logic circuit and its manufacture200118
US 2001049186 A1Method for establishing ultra-thin gate insulator using anneal in ammonia—10
US 2002011619 A1Semiconductor device having both memory and logic circuit and its manufacture—11
US 2002014700 A1Method and system for forming film, semiconductor device and fabrication method thereof—11
WO 0,223,614 A1Method for film formation of gate insulator, apparatus for film formation of gate insulator, and cluster tool—46
US 6,365,518 B1Method of processing a substrate in a processing chamber200266
US 2002047202 A1Semiconductor wafer assemblies comprising photoresist over silicon nitride materials—7
US 6,380,056 B1Lightly nitridation surface for preparing thin-gate oxides200271
US 2002072183 A1A semiconductor memory device having a trench capacitor—3

Non-Patent Literature (5)

  • Ishikawa, et al. "Nitride-Sandwiched-Oxide Gate Insulator For Low Power CMOS", 0-7803-7463-X.02; 2002, p. 869-872, IEEE.
  • Kraft, et al., "Surface Nitridation of Silicon Dioxide With a High Density Nitrogen Plasma," J. Vac. Sci. Technol. B 15(4), Jul./Aug. 1997, pp. 967-970.
  • Krug, et al., "Low Energy Nitrogen Implantation Into Si and SiO2/Si," Nuclear Instruments and Methods in Physics Research b 175-177 (2001) pp. 694-698.
  • Mahapatra, et al., "Device Scaling Effects on Hot-Carrier Induced Interface and Oxide-Trapped Charge Distributions in MOSFET's." IEEE Transactions on Electron Devices, vol. 47, No. 4, Apr. 2000, pp. 789-796.
  • Matsushita, et al., "Novel Fabrication Process to Realize Ultra-Thin (EOT=0.7nm) and Ultra-Low Leakage SiON Gate Dielectrics." IEEE-2004 Symposium on VLSI Technology, Digest of Technical Papers.