Patents
US 6,444,752 B1#31997602 Most CitedExpiredUnited States (USPTO)Utility

Monovinylidene aromatic polymers with improved toughness and rigidity and a process for their preparation

3Forward Citations (#31997602 Global)
0.1/yrCitation Velocity (#41426384 Global)
1.12Citation PageRank (#35541244 Global)
24Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed are rubber-modified monovinylidene aromatic polymers with improved toughness and rigidity as well as a process for the preparation thereof. The polymer comprises: a) a monovinylidene aromatic polymer matrix, b) rubber particles dispersed therein, characterized in that the rubber particles are produced from a diene rubber having I) from 20 to 80 percent, based on the total weight of said rubber particles, of a high solution viscosity component having a viscosity value ranging from 110 to 500 centipoise and II) from 80 to 20 percent, based on the total weight of said rubber particles, of a low solution viscosity component having a viscosity value ranging from 1 to 100 centipoise, further characterized in that the ratio of solution viscosity of high solution viscosity component to the solution viscosity of low solution viscosity ranges from 1.1 to 500, wherein both components I and II have a 1,4 cis content of greater than 30 percent, and III) the rubber is grafted with monovinylidene aromatic polymer to the extent that there is at least 30 percent monovinylidene aromatic polymer present as grafts on the rubber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A rubber modified monovinylidene aromatic polymer comprising: a) a monovinylidene aromatic polymer matrix, b) rubber particles dispersed therein, characterized in that the rubber particles are produced from a diene rubber having I) from 20 to 80 percent, based on the total weight of said rubber particles, of a high solution viscosity component having a viscosity value ranging from 110 to 500 centipoise and II) from 80 to 20 percent, based on the total weight of said rubber particles, of a low solution viscosity component having a viscosity value ranging from 1 to 100 centipoise, further charac

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 2,727,884 AProcess of mass polymerization in vertical unmixed strata195589
US 3,668,162 ATreating polybutadiene19728
US 4,146,589 AMethod for preparing a monoalkenyl aromatic polyblend having a dispersed rubber phase as particles with a bimodal particle size distribution197947
US 4,153,645 AHigh-impact polystyrene and process for the production thereof197921
US 4,183,877 AHigh-impact polystyrene composition and production thereof198030
US 4,214,056 AMethod for preparing a monoalkenyl aromatic polyblend having a dispersed rubber phase as particles with a bimodal particle size distribution198029
EP 0,048,389 A1Impact-resistant thermoplastic moulding masses—14
US 4,334,039 AProcess for preparing polymeric polyblends having a rubber phase as particles with a bimodal particle size distribution198222
US 4,340,690 ACyclic organo carbonate and sulfite coupling agents for living polymers of conjugated dienes198210
US 4,340,691 ALinear organo carbonate coupling agents for living polymers of conjugated dienes198220
EP 0,096,447 A2Rubber reinforced polymers of monovinylidene aromatic compounds and a method for their preparation—29
JP S5924711 ARubber-modified graft thermoplastic resin composition—6
US 4,493,922 AImpact-resistant thermoplastic molding material198570
EP 0,152,752 A2Connection for fibre-reinforced plastic pipes—19
EP 0,158,258 A2Impact-resistant resinous compositions and method of making—12
US 4,585,825 AMonovinylidene aromatic polymer resins having added amounts of high molecular weight polymer1986105
US 4,666,987 AIn-mold polymerization of vinyl aromatic compound198795
US 4,752,819 ASemiconductor integrated circuit device having a carrier trapping trench arrangement198816
EP 0,418,042 A1Monovinylidene aromatic polymers with improved properties and process for their preparation—19
US 5,240,993 AProcess for the preparation of rubber-reinforced monovinylidene aromatic polymers199332
JP H075789 AFixing device—4
EP 0,825,208 A2Process for the preparation of stress-crack-resistant thermoplastic moldings—4
EP 0,832,904 A1Process for manufacturing rubber-reinforced vinyl-aromatic polymers—9
JP 2,762,722 B2ポリブタジエンゴム及びそれを用いた耐衝撃性ポリスチレン系樹脂19982