Patents
US 4,334,039 A#3581231 Most CitedExpiredUnited States (USPTO)Utility

Process for preparing polymeric polyblends having a rubber phase as particles with a bimodal particle size distribution

22Forward Citations (#3581231 Global)
0.5/yrCitation Velocity (#15142138 Global)
6.00Citation PageRank (#2465838 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a method for preparing improved monoalkenyl aromatic polyblends having a dispersed rubber phase as rubber particles having a bimodal particle size distribution and compositions thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A continuous mass polymerization for preparing monoalkenyl aromatic polyblends having a dispersed rubber phase as rubber particles having a bimodal rubber particle size distribution comprising, A. continuously mass polymerizing a first solution of an alkenyl aromatic monomer having dissolved therein about 2 to 15% by weight of a first diene rubber in a first reaction zone to a conversion of about 10 to 40% forming a partially polymerized first solution with said first diene rubber being dispersed as rubber particles having an average diameter of about 0.1 to 1.0 microns, B. continuously feed

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

PatentTitleYearCitations
US 4,826,920 AFilms of linear ethylene polymer, polystyrene, and high impact polystyrene19898
US 6,444,752 B1Monovinylidene aromatic polymers with improved toughness and rigidity and a process for their preparation20023
US 5,298,563 AProcess for preparing an impact resistant resin19947
US 4,767,833 ATransparent, impact-resistant, thermoplastic resin composition having excellent chemical resistance and process for producing same198845
US 6,900,254 B2Processes for preparing impact modifier powders200515
US 6,660,798 B1Mixtures of fluoropolymer dispersions200318
US 5,179,166 AMonovinylidene aromatic polymers with improved properties and a process for their preparation19936
US 5,240,993 AProcess for the preparation of rubber-reinforced monovinylidene aromatic polymers199332
US 6,579,946 B2Low-gloss biaxially oriented films comprising vinyl aromatic polymers and substantially non-spherical rubber particles20039
US 6,815,500 B1Shock vinylaromatic polymer by polymerization of a vinylaromatic monomer in the presence of free radical and a polymerization initiator200411
EP 0,096,447 A3Rubber reinforced polymers of monovinylidene aromatic compounds and a method for their preparation—0
US 5,041,498 ATrimodal ABS compositions having good gloss and reduced gloss sensitivity199126
US 2002072552 A1Processes for preparing impact modifier powders—15
US 5,264,492 AMonovinylidene aromatic polymers with improved properties199310
US 2003055177 A1Monovinylidene aromatic polymers based on highly linear high molecular weight polybutadiene rubbers and a process for their preparation—14