Semiconductor manufacturing process and semiconductor device
Abstract
A tungsten film 20 is formed over a titanium-base film 18 to provide an interconnecting layer 22. An anti-reflection film 26 is formed over the interconnecting layer 22. Further, a photoresist 28 is applied over the anti-reflection film 26, followed by patterning. Using a mixed gas of SF6 and Cl2, the anti-reflection film 26 is etched. With a mixed gas of SF6 and Cl2, the tungsten film 20 is then etched. After that, the titanium-base film 18 is etched using a mixed gas of Cl2 and BCl3.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing a semiconductor device, the method comprising etching a composite of a titanium-base film under a tungsten film by: etching said tungsten film with a mixed gas of SF 6 and Cl 2 ; and then etching said titanium-base film with a mixed gas of Cl 2 and BCl 3 .
- Claim 2Depends on #1
The method for manufacturing a semiconductor device according to claim 1 , wherein: in said etching step of said tungsten film, flow of BCl 3 into an etching chamber is inhibited; and in said etching step of said titanium-base film, flow of SF 6 into said etching chamber is inhibited.
- Claim 3Depends on #1
The method for manufacturing a semiconductor device according to claim 1 , wherein in said etching step of said titanium-base film, BCl 3 is added at a flow rate of from 10 sccm to 40 sccm to Cl 2 .
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.