Abstract

After a contact hole is formed in an insulating film covering the surface of a semiconductor substrate, a Ti layer and a TiON (or TiN) layer are sequentially formed on the insulating film. On the TiON layer an Al alloy layer 18 containing Si is formed, and a reflow thermal treatment is performed after or during the formation of the Al alloy layer in order to improve step coverage. During this thermal treatment, Si nodules are generated. After a Ti layer is formed on the reflowed Al alloy layer, an annealing thermal treatment is performed for 120 seconds at a temperature of 450° to 500° C. With this thermal treatment, Si of Si nodules is absorbed in the Ti layer so that Si nodules are reduced or extinguished. After an antireflection TiN (or TiON) layer is formed on the Ti layer, wiring patterns are formed by using resist patterns as a mask. Since Si nodules are extinguished, wiring resistance can be reduced and an etching time can be shortened.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 12.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a semiconductor device comprising the steps of: (a) forming an Al alloy layer containing Si on a surface of a semiconductor substrate having a step; (b) heating and reflowing said Si containing Al alloy layer; (c) forming a Ti layer on said reflow Si containing Al alloy layer; (d) after step (c), annealing said semiconductor substrate at a temperature sufficient to consume any Si precipitates which may have been generated during said heating and reflowing step in said Si containing Al alloy layer; and (e) after the annealing step, patterning said Si containing

  2. Claim 2Depends on #1

    A method according to claim 1, wherein a temperature of said annealing step is higher than a temperature of said reflowing step.

  3. Claim 3Independent Claim

    A method according to c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • S. Wolf, "Silicon Processing for the VLSI Era, vol. 2", Lattice Press, p. 128, 1990.
  • S. Wolf, Silicon Processing for the VLSI Era, vol. 2 , Lattice Press, p. 128, 1990.