Patents
US 6,399,487 B1#4934276 Most CitedExpiredUnited States (USPTO)Utility

Method of reducing phase transition temperature by using silicon-germanium alloys

18Forward Citations (#4934276 Global)
0.8/yrCitation Velocity (#9862696 Global)
2.97Citation PageRank (#7689880 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An improved SALICIDE process is described wherein the transformation temperature to a lower resistivity suicide structure is reduced by first coating with a layer of a silicon-germanium alloy prior to the deposition of the titanium layer. Provided there is at least 40 atomic percent of germanium in the alloy a second RTA at a temperature no higher than about 650° C. may be effectively used. The resulting ternary alloy has a resistivity of about 15-20 microhm cm which corresponds to a sheet resistance of about 3-3.5 ohms per square. The ability to achieve low sheet resistance after annealing at such a low temperature becomes increasingly more important as device dimensions decrease since the second RTA becomes increasingly more likely to result in agglomeration of the silicidelayer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A selective contacting process comprising: providing a silicon body having a top surface which includes at least one area of silicon oxide; depositing a layer of silicon-germanium alloy, containing between 50 and 69.9 atomic percent of germanium, on the silicon top surface; depositing a layer of titanium on said silicon-germanium layer; subjecting the silicon body to a first rapid thermal anneal, thereby causing the titanium that is in contact with said silicon-germanium layer to form a layer of titanium-silicon-germanium alloy having a first sheet resistance value; selectively removing all un

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 10,964,544 B2Contact integration and selective silicide formation methods20210
US 9,269,570 B2Contact on a heterogeneous semiconductor substrate20163
US 2008194110 A1Methods of fabricating a semiconductor device using a dilute aqueous solution of an ammonia and peroxide mixture—1
US 10,103,028 B2Contact integration and selective silicide formation methods20183
FR 2,856,843 A1Procede de protection d'un element d'un circuit integre contre la formation d'un siliciure de metal—0
US 6,517,235 B2Using refractory metal silicidation phase transition temperature points to control and/or calibrate RTP low temperature operation20034
US 7,354,868 B2Methods of fabricating a semiconductor device using a dilute aqueous solution of an ammonia and peroxide mixture20084
EP 1,494,270 A1Process of protecting an element of an integrated circuit against silicide formation—0
US 2005186701 A1Method of protecting an element of an integrated circuit against the formation of a metal silicide—0
US 2005260830 A1Methods of fabricating a semiconductor device using a dilute aqueous solution of an ammonia and peroxide mixture—6
US 7,018,865 B2Method of protecting an element of an integrated circuit against the formation of a metal silicide20062
US 2017243760 A1Semiconductor device and manufacturing method thereof—33
EP 2,650,911 A1Contact point on a heterogeneous semiconductor substrate—0
US 10,522,368 B2Semiconductor device and manufacturing method thereof20194
US 8,058,180 B2Methods of fabricating a semiconductor device using a dilute aqueous solution of an ammonia and peroxide mixture20110

Non-Patent Literature (1)

  • Zhang et al., On the Intrinsic Spacer Layer in Si/SiGe Heterojunction Bipolar Transistor Grown by Ultra High Vacuum Chemical Vapor Deposition. 1997 IEEE/Cornell Conf. on Advanced Concepts in High Speed Semiconductor Devices and Circuits, 8/97. P.109-115.