hottub.patents
US 7,018,865 B2#950264 Most CitedExpiredUnited States (USPTO)Utility

Method of protecting an element of an integrated circuit against the formation of a metal silicide

0Forward Citations (#950264 Global)
0.0/yrCitation Velocity (#950264 Global)
0.97Citation PageRank (#950264 Global)
6Prior Art Cited
3Structured Claims
0Drawings / Sheets

Abstract

A semiconductor material is protected against the formation of a metal silicide by forming a layer of a silicon/germanium alloy on the material. The material which is protected belongs to a component of an integrated circuit comprising other components that have to be subjected to a siliciding operation. The method of protection includes depositing a layer of silicon/germanium alloy on the integrated circuit. The layer of silicon/germanium alloy is then removed from the areas to be silicided. A metal is then deposited on the structure and a metal silicide is formed therefrom. The unreacted metal and the metal/silicon/germanium ternary alloy that may have formed are removed, and the layer of silicon/germanium alloy is removed so as to expose the unsilicided component.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.

Claims (3)

  1. Claim 1Independent Claim

    A method of protecting a semiconductor material against the formation of a metal silicide, comprising: forming a layer of a silicon/germanium alloy on the semiconductor material; and selectively removing the silicon/germanium alloy from a certain portion of the silicon material to allow for silicidation of that certain portion while retaining the silicon/germanium alloy on another portion of the semiconductor material to protect against silicidation of that another portion.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the thickness of the layer of silicon/germanium alloy is greater than about 50 Å.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein the thickness of the layer of silicon/germanium alloy is around 200 Å.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (6)

PatentTitleYearCitations

Non-Patent Literature (1)

  • French Preliminary Search Report, FR 03 07690, dated Mar. 3, 2004.