Heat treatment for aluminum casting alloys to produce high strength at elevated temperatures
Abstract
An aluminum casting of composition that is hardenable due to the presence of suitable amounts of silicon, magnesium and, optionally, other hardening constituents such as copper, nickel and the like is heat treated for improved tensile strength at 300° C. The casting, which as formed has a microstructure of aluminum rich dendrites, silicon particles and hardening particles, is reheated above 500° C. to redissolve the hardening particles and redistribute hardening constituents through the aluminum dendrites, cooling the casting to 350° C. to 450° C. and holding there to reform an abundance of large stable hardening precipitates in the aluminum dendrites and then air cooling the casting. The thus treated casting may then be artificially age hardened such as by a T5 temper practice.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of increasing the tensile strength at 300° C. of an aluminum alloy casting, said casting consisting essentially, by weight, of 4 to 20% silicon, aluminum, 0.1 to 2% magnesium as a required hardening constituent and 0 to 4% copper, 0.2 to 2% iron, 0 to 3% nickel as optional hardening constituents, the microstructure of said casting comprising aluminum dendrites, silicon particles and hardening particles containing magnesium and said other hardening constituents if present, said method comprising (a) heating the casting to a temperature of about 500° C. to 540° C. to redissolve at least
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗