Method for producing cast alloy and magnet
Abstract
The magnetic properties of rare earth magnet are improved by means of forming a novel structure of the cast alloy used for the production of a rare earth magnet, which contains from 27 to 34% by weight of at least one rare earth element (R) including yttrium, from 0.7 to 1.4% by weight of boron, and the balance being essentially iron and, occasionally any other transition element, and comprises an R2T14B phase, an R-rich phase and optionally at least one ternary phase except for the R2T14B phase and the R-rich phase. The novel structure is that the volume fraction (V) in percentage of said R2T14B phase and said at least one ternary phase is more than 138-1.6r (with the proviso that r is the content of R), the average grain size of the R2T14B phases is from 10 to 100 mu m and, further, the average spacing between the adjacent R-rich phases is from 3 to 15 mu m. The novel structure can be formed by by means of feeding alloy melt onto a rotary casting roll, cooling in a temperature range of from melting point to 1000 DEG C. at a cooling rate of 300 DEG C. per second or more, and further cooling in a temperature range of from 800 to 600 DEG C. at a cooling rate of 1 DEG C./second or le
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 17.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of producing a cast alloy, comprising: feeding a melt onto a rotary casting roll, the melt comprising from 27 to 34% by weight of at least one element selected from the group consisting of the rare earth elements (R) and yttrium, from 0.7 to 1.4% by weight of boron, with the balance being essentially iron, and optionally other transition elements; cooling the melt in a temperature range of from melting point to 1000° C. at a cooling rate of 300° C. per second or more; and further cooling in a temperature range of from 800° C. to 600° C. at a cooling rate of 0.80° C./second or less.
- Claim 2Depends on #1
A method according to claim 1, wherein the cooling rate in the temperature range of from melting point to 1000° C. is 500° C. per second or more, and, further the cooling rate in the temperature range of from 800° C. to 600° C. is 0.75° C. per seco
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (3)
- Patent Abstracts of Japan vol. 013, No. 166 (E 746), Apr. 20, 1989 & JP 64 000706 A (Tokin Corp.), Jan. 5, 1989.
- Patent Abstracts of Japan vol. 013, No. 166 (E-746), Apr. 20, 1989 & JP 64 000706 A (Tokin Corp.), Jan. 5, 1989.
- Patent Abstracts of Japan vol. 095, No. 010, Nov. 30, 1995 & JP 07 176414 A (TDK Corp), Jul. 14, 1995.