Process for manufacturing permanent magnet
Abstract
A process for manufacturing a rare earth-iron-boron alloy permanent magnet by, after sintering, keeping the sintered alloy at temperatures of 750°-1000° C. for 0.2-5 hours, slowly cooling it at a cooling rate of 0.3°-5° C./min. to temperatures between room temperature and 600° C.; annealing it at temperatures of 550°-700° C. for 0.2-3 hours, and rapidly cooling it at a cooling rate of 20°-400° C./min. The permanent magnet contains a matrix, a B-rich phase and a Nd-rich phase. In grain boundaries of the matrix phases covered by bcc phases, thin, fine plates of the bcc phases projecting into the matrix phases are once increased by the first heat treatment and slow cooling and then eliminated by the annealing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 26.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for manufacturing a sintered body of a permanent magnet having an alloy composition represented by the general formula R(Fe.sub.1-x-y Co.sub.x B.sub.y)z wherein R represents Nd and/or Pr which may be partially substituted by one or more other rare earth elements, 0≦x≦0.5, 0.02≦y≦0.3 and 4≦z≦7.5, which comprises the steps of: (a) maintaining a sintered alloy body at temperatures of 750°-1000° C. for 0.2--5 hours after sintering; (b) cooling said sintered alloy body slowly at a cooling rate of 0.6°-2.0° C./min. to temperatures between room temperature and 600° C.; (c) annea
- Claim 2Independent Claim
The process for manufacturing a sintered body of a permanent magnet ac