Abstract

An activated porous phosphorus/vanadium oxide catalyst adapted for the catalytic oxidation of a hydrocarbon to produce a carboxylic acid anhydride. The catalyst comprises a shaped body having a volume of at least about 0.02 cc, a phosphorus content of between about 1.05 and about 1.20, a B.E.T. surface area of at least about 15 m2/g, an average vanadium oxidation state of between about 4.06 and about 4.3, a total pore volume of at least about 0.15 cc/g, a normalized apparent shaped body density of between about 1.0 and about 2.0 g/cc, and a crush strength of at least about 4 pounds. At least about 20% of the pore volume of the catalyst is constituted of pores having a diameter between about 0.1 and about 3.3 mu M, and at least about 40% of the pore volume is constituted of pores having a diameter of less than about 0.1 mu M. The catalyst is prepared by mixing a particulate phosphorus/vanadium oxide precursor with a pore modification agent to produce a modified catalyst precursor composition, forming the modified precursor composition into a predetermined shape, and removing the pore modification agent substantially at a temperature below 300 DEG C., preferably using air as a stripp

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 20.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of a phosphorus/vanadium oxide catalyst comprising the steps of: preparing a modified catalyst precursor composition comprising a mixture of a particulate phosphorus/vanadium oxide catalyst precursor and a volatile pore modification agent in proportions sufficient to provide a pore modification agent concentration of between about 8% and about 16% by weight, said pore modification agent having a vapor pressure of at least about 1 mm Hg at a temperature between about 150° C. and about 250° C. and being subject to vaporization, decomposition and/or oxidation at a te

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Brunauer et al., "Absorption of Gases in Multimolecular Layers," J. Am. Chem. Soc., vol. 60, pp. 309-319, 1938 (no month).
  • Brunauer et al., Absorption of Gases in Multimolecular Layers, J. Am. Chem. Soc., vol. 60, pp. 309 319, 1938 (no month).
  • Zazhigalov et al., "Effect of the Pore Structure and Granule Shape of V-P-O Catalyst of the Selectivity of Oxidation of n-Butane," Plenum Publishing Corp., pp. 97-101, 1988 (no month).
  • Zazhigalov et al., Effect of the Pore Structure and Granule Shape of V P O Catalyst of the Selectivity of Oxidation of n Butane, Plenum Publishing Corp., pp. 97 101, 1988 (no month).