Phosphorus-vanadium-oxygen catalysts having a specific pore volume
Abstract
The prior art discloses that phosphorus-vanadium-oxygen catalysts wherein the phosphorus to vanadium atom ratio is between about 1:2 and about 2:1, and wherein at least about 20 atom percent of the vanadium is in the tetravalent state, are useful for the conversion of aliphatic hydrocarbons to maleic anhydride. It has now been found that when the pore volume of the catalysts from pores having diameters between about 0.8 micron and about 10 microns is greater than 0.02 cc/g, the catalyst is particularly useful for the conversion of saturated hydrocarbons, such as butane, to maleic anhydride.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 48.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
In a method of preparing a phosphorus-vanadium-oxygen catalyst wherein a phosphorus compound and a vanadium compound are brought together under conditions to provide a catalyst precursor having a phosphorus to vanadium atom ratio between about 0.5:1 and 2:1, and calcining the precursor at a temperature between about 300° and 600° C., the improvement which comprises adding to the precursor a sufficient amount of a pore modification agent selected from the group consisting of polymeric materials, cellulosic materials, monosaccharides, polysaccharides, hydrogenated vegetable oils and mixtures the
- Claim 2Depends on #1
In a method of claim 1 wherein from about 1 weight percent to about 30 weight percent, b
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗