US 5,601,775 A#1959415 Most CitedExpiredUnited States (USPTO)Utility

Process for making an abrasion resistant quasi monofilament

33Forward Citations (#1959415 Global)
1.1/yrCitation Velocity (#5452573 Global)
4.06Citation PageRank (#4648131 Global)
23Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A quasi monofilament having a high strength polyethylene fiber core with an adherent, abrasion resistant polymer sheath is prepared by feeding the core yarn through a crosshead die, while simultaneously supplying a polymer melt at a temperature greater than the melting point of the core yarn to the die, for sheathing the core yarn within the die with the melt under a sufficient pressure to cause the melt to adhere to the core yarn. The abrasion resistant polymer sheath includes an effective amount of a first polymer having ethylene crystallinity, a density of at least about 0.94 g/cm 3 , and a melt index of less than about 0.1 g/10 min. The composition used to sheathe the core yarn is characterized by a weight average tensile strength at yield of greater than about 13.8 MPa. The quasi monofilament has utility in applications subjected to high abrasion, such as sports fishing lines, kite lines, dental floss, "weedeater" lines and tennis racket strings.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 33.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for making an abrasion resistant quasi monofilament, comprising the steps of: a. continuously feeding a core polyethylene multi-filament yarn having a tenacity of at least about 15 g/d and a tensile modulus of at least about 500 g/d through a crosshead die, while simultaneously b. supplying a polymer melt at a temperature greater than the melting point of the core yarn to the die, for c. sheathing the core yarn within the die with the melt under a sufficient pressure to cause the melt to adhere to the core yarn; and d. cooling the sheathed yarn to below the melting point of the

  2. Claim 2Depends on #1

    The process of claim 1 wherein the yarn is fed at a yarn velocity of up to about 900 m/min, the yarn has a residence time in the die of up to about 0.10 sec., and the melt is supplied at a melt throughput sufficient to form from abou

Technical Overview & Description