Process for the preparation of filaments of high tensile strength and modulus
Abstract
The invention relates to the preparation of filaments with a high tensile strength and a high modulus and to the filaments thus prepared. A solution of a linear polyethylene with a weight-average molecular weight of at least 4×10 5 is spun and the filaments, from which the solvent may have been removed in whole or in part, are drawn using a draw ratio of at least (12×10 6 /M w )+1. The filaments are drawn at a temperature such that the modulus is at least 20 GPa. The invention allows filaments to be prepared at high drawing rates, of 0.5 sec -1 or more, with a modulus of at least 20 GPa and a tensile strength of at least 1 GPa.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 106.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for the preparation of polyethylene filaments of high modulus and tensile strength which comprises spinning a solution having a concentration of from 1% to 20% by weight of a high-molecular-weight linear polyethylene polymer with a weight-average molecular weight of M w of at least 8×10 5 , and thereafter drawing the spun filaments using a draw ratio of at least (12×10 6 /M w )+1, at a drawing temperature of between 75° to 135° C. such that, at the draw ratio, concentration and temperature used, the modulus of the filaments is at least 20 GPa.
- Claim 2Independent Claim
A process for the preparation of polyethylene filaments of high modulus and tensile strength which consists essentially in spinning a solution having a concentration of from 1% to 20% of high molecular weight linear polyethylene polymer, said polymer having a weight-average molec
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗