Mold process for syndiotactic polypropylene
Abstract
A molding process for syndiotactic polypropylene includes holding the melt at a process temperature of about 27 DEG to 77 DEG C. to achieve a cycle time of less than 150 DEG C. and a haze value for a 2 mm thick article of less than 38%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for molding syndiotactic polypropylene comprising: a) injecting a melt of syndiotactic polypropylene into a mold maintained at a temperature sufficient to keep said melt in the mold at a process temperature of 49° to 77° C.; b) holding said melt at said process temperature until it crystallizes into an article having the shape of said mold; and c) ejecting said article from said mold wherein process steps (a) and (b) are complete in a cycle time of 50 sec. or less and said article has a haze value of 31% or less.
- Claim 2Depends on #1
The process of claim 1 wherein said melt is at a temperature of at least 200° C. when injected into said mold.
- Claim 3Depends on #1
The process of claim 1 wherein said melt includes a polymer additive.