Process for injection molding
Abstract
A process for preparing a low haze molded article includes adding a nucleating agent to a polypropylene homopolymer or copolymer to form prenucleated polypropylene having a molecular weight of at least about 20,000 and an isotactic index of at least about 60 percent, and forming a molding composition by mixing the prenucleated polypropylene with linear low density polyethylene having a melt index of at least about 120 grams per 10 minutes, in an amount of about 1 to 5 percent by weight based on the total weight of the polyethylene and the polypropylene. This mixture is then introduced into an injection molding zone where it is molded at a temperature below the melting point of the polypropylene.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 9.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for preparing a low haze molded article comprising: (i) adding a nucleating agent to a polypropylene homopolymer or copolymer to provide a prenucleated polypropylene homopolymer or copolymer having a molecular weight of at least about 20,000 and an isotactic index of at least about 60 percent; (ii) forming a composition by mixing the prenucleated polypropylene with linear low density polyethylene having a melt index of at least about 120 grams per 10 minutes, in an amount of about 1 to about 5 percent by weight based on the total weight of the polyethylene and the polypropylene;
- Claim 2Depends on #1
The process defined in claim 1 wherein the linear low de
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗